KCl--ZnCl2沉积盐导致Fe--15Cr--xAl合金表面氧化铬膜的退化
潘太军1 ; 胡静 1 ; 牛焱2
1.江苏工业学院材料科学与工程学院 常州高分子新材料重点实验室 常州 213164
2.中国科学院金属研究所 金属腐蚀与防护国家重点实验室 沈阳 110016
Degradation of the chromia on Fe--15Cr--xAl alloy induced by KCl--ZnCl2 deposits
PAN Taijun 1 ; HU Jing 1 ; NIU Yan 2
1.Department of Materials Science and Engineering; Jiangsu Polytechnic University; Key Laboratory for Polymer Materials; Changzhou; 213164
2.State Key Laboratory for Corrosion and Protection; Institute of Metal Research; the Chinese Academy of Science; Shenyang 110016
引用本文:

潘太军 胡静 牛焱. KCl--ZnCl2沉积盐导致Fe--15Cr--xAl合金表面氧化铬膜的退化[J]. 材料研究学报, 2009, 23(4): 347-351.
. Degradation of the chromia on Fe--15Cr--xAl alloy induced by KCl--ZnCl2 deposits[J]. Chin J Mater Res, 2009, 23(4): 347-351.

全文: PDF(949 KB)  
摘要: 

研究了三种Fe--15Cr--xAl(x=0, 5, 10, 原子分数)合金在600℃于ZnCl2--KCl盐膜下的腐蚀行为. 与氧化相比, 所有合金在盐膜下均发生加速腐蚀, 生成了疏松多孔的腐蚀产物膜, 且发生内腐蚀. 合金的腐蚀速率随着铝含量的增加而降低. 铝的作用主要是由于Al2O3在腐蚀产物内层富集, 充当阻挡层有效地阻碍了反应介质在膜中的传递.

关键词 材料失效与保护Fe--Cr--AlKCl--ZnCl2 热腐蚀    
Abstract

The corrosion behavior of three Fe--15Cr--xAl(x=0, 5, 10%) alloys below KCl--ZnCl2 deposits in air was investigated at 600℃. Compared to their oxidation in air, all the alloys suffered from enhanced corrosion with the formation of non--protective porous scale, particularly in combination with internal attack of matrix. The corrosion rates decreased with increasing aluminum content. The effect of aluminum was mainly attributed to the enrichment of Al2O3 in the inner region of the scale, which may act as a barrier by retarding the rapid migration of the reactants.

Key wordsmaterials failure and protection    Fe--Cr--Al    KCl--ZnCl2    hot corrosion
收稿日期: 2008-11-23     
ZTFLH: 

TB304

 
基金资助:

国家自然科学基金50671114项目、江苏省高校自然科学基金08KJB430003项目和常州市工业科技攻关CE2008089项目资助.

1 Y.Kawahara, High temperature corrosion mechanisms and effect of alloying elements for materials used in waste incineration environment, Corrosion Science, 44, 223(2002)
2 T.Ishitsuka, K.Nose, Stability of protective oxide films in waste incineration environment–solubility measurement of oxides in molten chlorides, Corrosion Science, 44, 247(2002)
3 A.Zahs, M.Spiegel, H.J.Grabke, The influence of alloying elements on the chlorine induced high temperature corrosion of Fe–Cr alloys in oxidizing atmospheres, Materials and Corrosion, 50, 561(1999)
4 H.Fujikawa, N.Maruyama, Corrosion behavior of austenitic stainless steels in the high chloride–containing environment, Materials Science and Engineering, A120, 301(1989)
5 P.F.Tortorelli, K.Natesan, Critical factors affecting the high–temperature corrosion performance of iron aluminides, Materials Science and Engineering, A258, 115(1998)
6 Y.S.Li, M.Spiegel, Models describing the degradation of FeAl and NiAl alloys induced by ZnCl2–KCl melt at 400–450  , Corrosion Science, 46, 2009(2004)
7 Y.S.Li, M.Spiegel, S.Shimada, Effect of Al/Si addition on KCl induced corrosion of 9% Cr steel, Materials Letters, 58, 3787 (2004)
8 R.A.Rapp, The transition from internal to external oxidation and the formation of interruption bands in Silver– indium alloys, Acta Materialia, 9, 730 (1961)
9 F.H.Stott, J.F.Norton, Laboratory studies involving corrosion in complex, multi–component gaseous environments at elevated temperatures, Materials at High Temperature, 14, 109(1997)
10 Y.Niu, F.Gesmundo, An approximate analysis of the external oxidation of ternary alloys forming insoluble oxides , Oxidation of Metals, 56, 517(2001)
11 M.Spiegel, Salt melt induced corrosion of metallic materials in waste incineration plants, Materials and Corrosion, 50, 373(1999)
12 Y.S.Li, M.Spiegel, 6th International Symposium on High Temperature Corrosion and Protection of Materials, Les Embiez, France, May 16–21(2004)

[1] 高巍, 刘江南, 魏敬鹏, 要玉宏, 杨巍. TC4钛合金表面氧化亚铜掺杂微弧氧化层的结构和性能[J]. 材料研究学报, 2022, 36(6): 409-415.
[2] 杨留洋, 谭卓伟, 李同跃, 张大磊, 邢少华, 鞠虹. 利用WBEEIS测试技术对管道缺陷区动态冲刷腐蚀行为的研究[J]. 材料研究学报, 2022, 36(5): 381-391.
[3] 陈铮, 杨芳, 王成, 杜瑶, 卢壹梁, 朱圣龙, 王福会. 惰性无机填料比例和颗粒尺寸对纳米Al/Al2O3 改性有机硅涂料抗高温氧化行为的影响[J]. 材料研究学报, 2022, 36(4): 271-277.
[4] 李玉峰, 张念飞, 刘丽爽, 赵甜甜, 高文博, 高晓辉. 含磷石墨烯的制备及复合涂层的耐蚀性能[J]. 材料研究学报, 2022, 36(12): 933-944.
[5] 陈艺文, 王成, 娄霞, 李定骏, 周科, 陈明辉, 王群昌, 朱圣龙, 王福会. 无机复合涂层对CB2铁素体耐热钢在650℃水蒸气中的防护[J]. 材料研究学报, 2021, 35(9): 675-681.
[6] 唐荣茂, 刘光明, 刘永强, 师超, 张帮彦, 田继红, 甘鸿禹. 用电化学噪声技术研究Q235钢在含氯盐模拟混凝土孔隙液中的腐蚀行为[J]. 材料研究学报, 2021, 35(7): 526-534.
[7] 张大磊, 魏恩泽, 荆赫, 杨留洋, 豆肖辉, 李同跃. 超级铁素体不锈钢表面超疏水结构的制备及其耐腐蚀性能[J]. 材料研究学报, 2021, 35(1): 7-16.
[8] 王冠一, 车欣, 张浩宇, 陈立佳. Al-5.4Zn-2.6Mg-1.4Cu合金板材的低周疲劳行为[J]. 材料研究学报, 2020, 34(9): 697-704.
[9] 黄安然, 张伟, 王学林, 尚成嘉, 范佳杰. 铁素体不锈钢在高温尿素环境中的腐蚀行为研究[J]. 材料研究学报, 2020, 34(9): 712-720.
[10] 公维炜, 杨丙坤, 陈云, 郝文魁, 王晓芳, 陈浩. 扫描电化学显微镜原位观察碳钢涂层缺陷处的交流腐蚀行为[J]. 材料研究学报, 2020, 34(7): 545-553.
[11] 郭铁明, 徐秀杰, 张延文, 宋志涛, 董志林, 金玉花. Q345q桥梁钢和Q345qNH耐候钢在模拟工业大气+除冰盐混合介质中的腐蚀行为[J]. 材料研究学报, 2020, 34(6): 434-442.
[12] 朱金阳, 谭成通, 暴飞虎, 许立宁. 一种新型含AlCr合金钢在模拟油田采出液环境下的CO2腐蚀行为[J]. 材料研究学报, 2020, 34(6): 443-451.
[13] 梁新磊, 刘茜, 王刚, 王震宇, 韩恩厚, 王帅, 易祖耀, 李娜. 氧化石墨烯改性环氧隔热涂层的耐蚀和隔热性能研究[J]. 材料研究学报, 2020, 34(5): 345-352.
[14] 王志虎,张菊梅,白力静,张国君. 水热处理对AZ31镁合金微弧氧化陶瓷层组织结构及耐蚀性的影响[J]. 材料研究学报, 2020, 34(3): 183-190.
[15] 段体岗, 黄国胜, 马力, 彭文山, 张伟, 许立坤, 林志峰, 何华, 毕铁满. Q235/Ni-Co基自修复涂层的制备和耐蚀性能[J]. 材料研究学报, 2020, 34(10): 777-783.