1240 MPa级Ti-38644高锁螺栓的拉伸疲劳增寿机理 |
赵庆云( ),程思锐,黄宏 |
中国航空制造技术研究院 北京 100024 |
|
Mechanism of Fatigue Life Enhancement for 1240 MPaHi-lock Bolt of Ti-38644 Ti-alloy |
ZHAO Qingyun( ),CHENG Sirui,HUANG Hong |
AVIC Manufacturing Technology Institute, Beijing 100024, China |
引用本文:
赵庆云,程思锐,黄宏. 1240 MPa级Ti-38644高锁螺栓的拉伸疲劳增寿机理[J]. 材料研究学报, 2019, 33(10): 735-741.
Qingyun ZHAO,
Sirui CHENG,
Hong HUANG.
Mechanism of Fatigue Life Enhancement for 1240 MPaHi-lock Bolt of Ti-38644 Ti-alloy[J]. Chinese Journal of Materials Research, 2019, 33(10): 735-741.
[1] | Zeng L, Haylock L, Fanning J ,et al. Evaluation of newly developed Ti-555 high-strength titanium fasteners [J]. www.alcoa.com | [2] | Fanning J, Zeng L, Nyakana S ,et al. Properties and microstructures of Ti-555(Ti-5Al-5Mo-5V-3Cr-0.6Fe) for fasteners [J]. Ti-2007 Science and Technology, 2007, 1263 | [3] | Fanning J. Properties of TIMETAL 555 (Ti-5Al-5Mo-5V-3Cr-0.6Fe) [J]. Journal of Materials Engineering and Performance, 2005,14(6): 788 | [4] | Technologies SPS. New SPS TitanTM titanium fasteners for high performance racing [J]. www.SPS.com. | [5] | Pang X C, Bai M Y. Fracture analysis of titanium alloy bolt [J]. Failure Analysis and Prevention, 2011, 6(3): 182 | [5] | 庞小超, 白明远.钛合金螺栓断裂原因分析 [J]. 失效分析与预防, 2011, 6(3): 182 | [6] | Gao Y K. Influence of shot peening on tension-tension fatigue properties in Ti-10V-2Fe-3Al titanium alloy [J]. The Chinese Journal of Nonferrous Metals, 2004, 14(1): 60 | [6] | 高玉魁. 喷丸对Ti-10V-2Fe-3Al钛合金拉拉疲劳性能的影响 [J]. 中国有色金属学报, 2004, 14(1): 60 | [7] | Chen J D, Liu Y, Tian F G, et al. The analysis of processes and the development of NC machine for rolling rounds of bolts[J], Manufactuing Automation, 2011, 33(12) : 72-75. | [7] | 陈家兑, 刘 勇, 田丰果等. 螺栓圆角滚压工艺分析及数控圆角滚压机研制 [J]. 制造业自动化, 2011, 33(12): 72 | [8] | Yu S F, Wang Z Q, Liu F Z. The cool-rolling equipment for making round of high-strength bolts [J]. Aviation Maintenance & Engineering, 1997, (5): 24 | [8] | 余述凡, 王自勤, 刘凤章. 高强度螺栓圆角冷挤机 [J]. 航空制造工程, 1997, (5): 24 | [9] | Chen W, Sun Q Y, Xiao L ,et al. Effect of duplex aging on low cycle fatigue behavior in Ti-10V-2Fe-3Al alloy [J]. Rare Metal Materials and Engineering, 2012, 41(11): 1911 | [9] | 陈 威, 孙巧艳, 肖 林等. 双重时效对Ti1023合金低周疲劳行为的影响 [J]. 稀有金属材料与工程, 2012, 41(11): 1911 | [10] | Zhan X D, Zhang X Y, Li S J, et al. Critical conditions of α lamellar crushing during hot deformation in Ti-55531 near-β titanium alloy [J]. Material Science and Engineering of Powder Metallugy, 2016, 21(5): 665 | [10] | 詹孝冬, 张晓泳, 李少君等. Ti-55531近β钛合金中针片α组织破碎的临界变形条件 [J]. 粉末冶金材料科学与工程, 2016, 21(5): 665 | [11] | Zhang Z J, Zhang P, Li L L,et al. Fatigue cracking at twin boundaries: Effects of crystallographic orientation and stacking fault energy [J]. Acta Materialia, 2012, 60(6-7): 3113 | [12] | Huang J, Wang Z R, Zhou J. Cyclic deformation response of β -annealed Ti-5Al-5V-5Mo-3Cr alloy under compressive loading conditions [J]. Metallurgical and Materials Transactions A, 2011, 42(9): 2868 | [13] | Bantounas I, Dye D, Lindley T C. The role of microtexture on the faceted fracture morphology in Ti-6Al-4V subjected to high-cycle fatigue [J]. Acta Materialia, 2010, 58(11): 3908 | [14] | Bantounas I, Dye D, Lindley T C. The effect of grain orientation on fracture morphology during high-cycle fatigue of Ti-6Al-4V [J]. Acta Materialia, 2009, 57(12): 3584 | [15] | Yang D M, Zhu X. Mechanical Properties and Failure Analysis of metals [M]. Beijing: Metallurgical Industry Press, 1991, 313. | [15] | 杨道明, 朱 勋. 金属力学性能与失效分析 [M]. 北京: 冶金工业出版社, 1991, 313 | [16] | Qin D, Lu Y, Liu Q ,et al. Transgranular shearing introduced brittlement of Ti-5Al-5V-5Mo-3Cr alloy with full lamellar structure at room temperature [J]. Materials Science Engineering A, 2013, 572(11): 19 | [17] | Zhong Q P, Tian Y J. Failure Analysis Basis [M]. Beijing: China Machine Press, 1990, 326 | [17] | 钟群鹏, 田永江. 失效分析基础知识 [M]. 北京: 机械工业出版社, 1990, 326 |
|
|