Corrosion Behavior of Q345q Steel with Oxide Scale in Simulated Typical Atmospheric Environmentin Northwest China |
ZHANG Yanwen1,2,GUO Tieming1,2( ),SONG Zhitao1,2,NAN Xueli1,2,XU Xiujie1,2,DONG Zhilin1,2 |
1. State Key Laboratory of Advanced Processing and Recycling of Non-ferrous Metals, Lanzhou University of Technology, Lanzhou 730050, China 2. School of Materials Science and Engineering, Lanzhou University of Technology, Lanzhou 730050, China |
|
Cite this article:
ZHANG Yanwen,GUO Tieming,SONG Zhitao,NAN Xueli,XU Xiujie,DONG Zhilin. Corrosion Behavior of Q345q Steel with Oxide Scale in Simulated Typical Atmospheric Environmentin Northwest China. Chinese Journal of Materials Research, 2019, 33(10): 749-762.
|
Abstract The structure of the oxide scale on the as received hot-rolled bridge steel Q345q and the corrosion behavior of the steel Q345q with oxide scale in three simulated atmospheric environments in Northwest China were studied by XRD, scanning electron microscopy, electrochemical technique and wet-dry alternating corrosion test. The results show that the hot-rolled oxide scale composes mainly of Fe3O4 and Fe2O3, which is porous with cracks and other defects. After the dry-wet alternating accelerated corrosion test of the steel Q345q with oxide scale, although the corrosion weight loss is the highest in NaHSO3 solution, the free-corrosion potential increases with the corrosion time, and the free-corrosion current density decreases in the later stage of corrosion. As far as the morphology of the rust layer and the ratio of γ/α* are concerned, the rust layer formed on the steel presents good stability; However, in deicing salt solution, the corrosion rate is the smallest, but the steel suffered mainly from Cl--dominated pitting corrosion with the corrosion characteristics of "large cathode and small anode". Its corrosion products contain such as β-FeOOH and HFeCl4(H2O)6, which results in loose rust layer with poor protectiveness and increased free-corrosive current density; In deicing salt+NaHSO3 solution, both pitting corrosion and general corrosion occur. Due to the synergistic effect of Cl- and HSO3-, the autocatalytic effect of a part of Cl- is reduced, but most α-FeOOH is converted from β-FeOOH, which resulted in the poor protective rust layer.
|
Received: 30 January 2019
|
|
Fund: National Natural Science Foundation of China(51461029);Guangdong Sailing Program to Introduce Innovative Entrepreneurial Team of Special Funding(2015YT02G090);Scientific Research Projects of Gansu Transportation Department(2017-16);Scientific Research Projects of Gansu Transportation Department(2017-19) |
[1] | Zhu Y J, Gao Y, Song Q J, et al. A brief description of current status and development trend for bridge structural steel plate [J]. Wide. Heavy. Plate, 2016, 22(3): 43 | [1] | 朱宜进, 高 雅, 宋庆吉等. 浅述桥梁钢的发展现状和趋势 [J]. 宽厚板, 2016, 22(3): 43 | [2] | Wang Y Z. Application situation and development of Chinese bridges steel structure [J]. Constr. Technol., 2010, 39(8): 13 | [2] | 王用中. 我国桥梁钢结构的应用现状与展望 [J]. 施工技术, 2010, 39(8): 13 | [3] | Wei J, Dong J H, Ke W. The influence of cooling processes on the corrosion performance of the rebar scale [J]. Constr. Build. Mater., 2010, 24(3): 275 | [4] | Pérez F J, Martínez L, Hierro M P ,et al. Corrosion behavior of different hot rolled steels [J]. Corros. Sci., 2006, 48(2): 472 | [5] | Han J K, Yan H, Hang Y ,et al. Structural features of oxide scales on weathering steel and their influence on atmospheric corrosion [J]. Acta Metall. Sin., 2017, 53(2): 163 | [5] | 韩军科, 严 红, 黄 耀等. 耐候钢表面氧化皮的结构特征及其对大气腐蚀行为的影响 [J]. 金属学报, 2017, 53(2): 163 | [6] | Dong C F, Xue H B, Li X G ,et al. Electrochemical corrosion behavior of hot-rolled steel under oxide scale in chloride solution [J]. Electrochim. Acta, 2009, 54(17): 4223 | [7] | Collazo A, Covelo A, Izquierdo M ,et al. Effect of the experimental setup in the behavior of sol-gel coatings [J]. Prog. Org. Coat., 2008, 63(3): 291 | [8] | Chattopadhyay A, Bandyopadhyay N, Das A K ,et al. Oxide scale characterization of hot rolled coils by Raman spectroscopy technique [J]. Scripta. Mater., 2005, 52(3): 211 | [9] | Zhang H M, Qi G T, Qiu Y B. Research on galvanic corrosion of carbon steel and oxide scales [J]. Oil-Gas Field Surf. Eng., 1995, 14(5): 32 | [9] | 张华民, 齐公台, 邱于斌. 氧化皮─碳钢电偶腐蚀研究 [J]. 油气田地面工程, 1995, 14(5): 32 | [10] | Zhang H M, Qi G T, Dai J B ,et al. Influence of high-temperature oxide scales on corrosion of steel substrate [J]. Mater. Prot., 1995,28(6): 24 | [10] | 张华民, 齐公台, 戴金彪等. 钢铁表面高温氧化皮对基体钢腐蚀的影响 [J]. 材料保护, 1995, 28(6): 24 | [11] | Zhou X L, Nie L, Hua X Z ,et al. Influence of heat treatment temperature on structure and corrosion resistance of oxide scales formed on hot-rolled steel 510L [J]. Mater. Heat. Treat., 2011, 32(10): 117 | [11] | 周贤良, 聂 轮, 华小珍等. 热处理温度对510L钢氧化皮结构及耐蚀性的影响 [J]. 材料热处理学报, 2011, 32(10): 117 | [12] | He A H. The effect of oxide film on the electrochemical corrosion behaviors of hot rolled steel [D]. Qingdao: Ocean University of China, 2007 | [12] | 何爱花. 热轧钢板氧化膜对基体碳钢腐蚀电化学行为的影响 [D]. 青岛: 中国海洋大学, 2007 | [13] | Zhang X, Yang S W, Zhang W H ,et al. Corrosion behavior of low-alloy weathering steel in cyclically alternate corrosion environments [J]. Chin. J. Mater. Res., 2013, 27(1): 18 | [13] | 张 旭, 杨善武, 张文华等.低合金耐候钢在周期性交替条件下的腐蚀行为 [J]. 材料研究学报, 2013, 27(1): 18 | [14] | Zhang D, Wang Z Y, Zhou Y Z ,et al. Initial corrosion behavior of galvanized steel in atmosphere by Qinghai salt lake [J]. Chin. J. Mater. Res., 2018, 32(4): 256 | [14] | 张 丹, 王振尧, 周永璋等. 镀锌钢在青海盐湖大气环境下的初期腐蚀行为研究 [J]. 材料研究学报, 2018, 32(4): 256 | [15] | Benarie M, Lipfert F L. A general corrosion function in terms of atmospheric pollutant concentrations and rain PH [J]. Atmos. Environ., 1986, 20(10): 1947 | [16] | Han W, Pan C, Wang Z ,et al. A study on the initial corrosion behavior of carbon steel exposed to outdoor wet-dry cyclic condition [J]. Corros. Sci., 2014, 88(16): 89 | [17] | Legault R A, Preban A G. Kinetics of the atmospheric corrosion of low-alloy steels in an industrial environment [J]. Corros., 1975, 31(4): 117 | [18] | Ma Y, Li Y, Wang F. The atmospheric corrosion kinetics of low carbon steel in a tropical marine environment [J]. Corros. Sci., 2010, 52(5): 1796 | [19] | Refait P, Génin J M R. The mechanisms of oxidation of ferrous hydroxychloride β-Fe2(OH)3 Cl in aqueous solution: The formation of akaganeite vs goethite [J]. Corros. Sci., 1997, 39(3): 539 | [20] | Evans U R, Taylor C A J. Mechanism of atmospheric rusting [J]. Corros. Sci., 1972, 12(3): 227 | [21] | Dillmann P, Mazaudier F, H?rlé S. Advances in understanding atmospheric corrosion of iron. I. Rust characterisation of ancient ferrous artefacts exposed to indoor atmospheric corrosion [J]. Corros. Sci., 2004, 46(6): 1401 | [22] | Asami K, Kikuchi M. In-depth distribution of rusts on a plain carbon steel and weathering steels exposed to coastal-industrial atmosphere for 17 years [J]. Corros. Sci., 2003, 45(11): 2671 | [23] | Kamimura T, Hara S, Miyuki H ,et al. Composition and protective ability of rust layer formed on weathering steel exposed to various environments [J]. Corros. Sci., 2006, 48(9): 2799 | [24] | Luo J. Influence of pre-oxidation on the corrosion behavior of weathering steel [D]. Beijing: University of Science and Technology Beijing, 2012 | [24] | 罗 娇. 预氧化对耐候钢腐蚀行为的影响 [D]. 北京:北京科技大学, 2012 | [25] | Qian Y H, Ma C H, Niu D ,et al. Influence of alloyed chromium on the atmospheric corrosion resistance of weathering steels [J]. Corros. Sci., 2013, 74: 424 | [26] | Fuente D D L, Díaz I, Simancas J ,et al. Long-term atmospheric corrosion of mild steel [J]. Corros. Sci., 2011, 53(2): 604 | [27] | Yamashita M, Miyuki H, Matsuda Y ,et al. The long term growth of the protective rust layer formed on weathering steel by atmospheric corrosion during a quarter of a century [J]. Cheminform, 1994, 25(19): 283 | [28] | Suzuki I, Masuko N, Hisamatsu Y. Electrochemical properties of iron rust [J]. Corros. Sci., 1979, 19(8): 521 | [29] | Bhattacharya A , Singh P M . Electrochemical behavior of duplex stainless steels in caustic environment [J]. Corros. Sci., 2011, 53(1): 71 | [30] | Quan B L, Li J Q, Chen C Y. Effects of sodium thiosulfate on corrosion dynamics of Q235 steel in alkaline environment [J]. Corros. Prot., 2018, 39(2): 103 | [30] | 权变利, 李军旗, 陈朝轶. 碱性环境中硫代硫酸钠对Q235钢腐蚀动力学的影响 [J]. 腐蚀与防护, 2018, 39(2): 103 | [31] | Chen H L, Li X J, Wei Y. Corrosion mechanism of carbon steel in chloride solution [J]. Corros. Prot., 2007, 28(1): 17 | [31] | 陈惠玲, 李晓娟, 魏 雨. 碳钢在含氯离子环境中腐蚀机理的研究 [J]. 腐蚀与防护, 2007, 28(1): 17 | [32] | Gao X L, Han Y, Fu G Q ,et al. Evolution of the rust layers formed on carbon and weathering steels in environment containing chloride ions [J]. Acta Metall. Sin. (Engl. Lett.), 2016, 29(11: 1025 | [33] | Fu M H. Research on structure and corrosion resistance of oxide scale of hot-strip steel [D]. Nanchang: Nanchang Hang Kong University, 2009 | [33] | 符明含. 热轧带钢氧化皮结构及耐腐蚀性能研究 [D]. 南昌: 南昌航空大学, 2009 | [34] | Ohtsuka T, Komatsu T. Enhancement of electric conductivity of the rust layer by adsorption of water [J]. Corros. Sci., 2005, 47(10): 2571 | [35] | Chen H L, Chen S H, Wei Y. Formation mechanism of Fe3O4 and α-FeOOH on carbon steel surface in 3%NaCl solution [J]. Mater. Prot., 2007, 40(9): 20 | [35] | 陈惠玲, 陈淑慧, 魏 雨. 3%NaCl溶液中碳钢表面Fe3O4和α-FeOOH的形成机理 [J]. 材料保护, 2007, 40(9): 20 |
|
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|