Abstract Ni3Si alloys were microalloyed via arc melting with small amounts of Cr and B for improving their mechanical properties. The microstructure, phase composition and tribological property of Ni3Si alloys were investigated. Results show that Ni3Si alloy was mainly composed of β1-Ni3Si and γ-Ni31Si12 phases; with the increasing Cr-conten the phase composition was changed to γ-Ni31Si12 and α-Ni, and then changed to γ-Ni31Si12 and Cr3Ni5Si2; the microhardness increased along with the increasing Cr-content; during the dry sliding friction the friction coefficients of the alloys were about 0.5 and their wear rates were much lower than that of 316 stainless steel. The optimum addition of Cr for the best tribological property of the Ni3Si alloy was 5% Cr (in mass fraction). With the increasing load the wear mechanisms of Ni3Si alloys with 0% and 5% Cr exhibited significant change from abrasive wear to adhesive wear. The wear mechanisms of the alloys with 10% Cr were all the fatigue wear within the range of the test load.
|
Received: 07 March 2017
|
Fund: Supported by Natural Science Fund for Colleges and Universities in Jiangsu Province (No. 15KJB460007), National Natural Science Foundation of China (No. 51505199) and Natural Science Foundation of Jiangsu Province (No. BK20140511) |
[1] | Kittl J A, Pawlak M A, Lauwers A, et al.Work function of Ni silicide phases on HfSiON and SiO2: NiSi, Ni2Si, Ni31Si12, and Ni3Si fully silicided gates[J]. IEEE Electron Device Lett., 2006, 27(1): 34 | [2] | Song Y, Jin S.Synthesis and properties of single-crystal β3-Ni3Si nanowires[J]. Appl. Phys. Lett., 2007, 90(17): 173122 | [3] | Sukidi N, Koch C C, Liu C T.The oxidation of Ni3Si-base alloys[J]. Mater. Sci. Eng. A, 1995, 191(1-2): 223 | [4] | Takasugi T, Kawai H,Kaneno Y. The effect of Cr addition on mechanical and chemical properties of Ni3Si alloys [J]. Mater. Sci. Eng. A, 2002, 329-331: 446 | [5] | Bi Q L, La P Q, Liu W M, et al.Microstructure and properties of Ni3Si alloyed with Cr fabricated by self-propagating high-temperature synthesis casting route[J]. Metall. Mater. Trans. A, 2005, 36: 1301 | [6] | Takasugi T, Suenaga H,Izumi O.Environmental effect on mechanical properties of recrystallized L12-type Ni3(Si,Ti) intermetallics[J]. J. Mater. Sci., 1991, 26(5): 1179 | [7] | Liu C T,Oliver W C.Environmental embrittlement and grain-boundary fracture in Ni3Si[J]. Scripta Metall. Mater., 1991, 25(8): 1933 | [8] | Zhu J H, Liu C T.Intermediate-temperature mechanical properties of Ni-Si alloys: oxygen embrittlement and its remedies[J]. Intermetallics, 2002, 10(4): 309 | [9] | Cui C, Xue T, Jin Y, et al.Tensile and fatigue behaviour of Ni-Ni3Si eutectic in situ composites[J]. Mater. Sci. Technol., 2016, 32(10): 1053 | [10] | Takasugi T, Hanada S. The influence of second-phase dispersion on environmental embrittlement of Ni3(Si, Ti) alloys [J]. MRS Proceedings, 1998, 552: KK6.5.1 | [11] | Takasugi T, Kawai H, Kaneno Y.Mechanical and chemical properties of Ni3Si and Ni3(Si,Ti) alloys multiphased by chromium addition[J]. Mater. Sci. Technol., 2001, 17: 671 | [12] | Takasugi T,Yoshida M.The effect of Nb addition on microstructure and mechanical properties of Ni3(Si,Ti) alloy[J]. J. Mater. Sci., 2001, 36(3): 643 | [13] | Van Dyck S, Delaey L, Froyen L, et al.Reactive powder metallurgy of Ni3Si-based alloys[J]. Intermetallics, 1995, 3(4): 309 | [14] | Ahmad R, Cochrane R F, Mullis A M.The formation of regular αNi-γ(Ni31Si12) eutectic structures from undercooled Ni-25at.% Si melts[J]. Intermetallics, 2012, 22: 55 | [15] | Gladyshevskii E I,Borusevich L K.The Cr-Ni-Si Ternary System[J]. Russian J. Inorg. Chem., 1963, 8(8): 997 | [16] | Guard R W,Smith E A.Constitution of Ni-base Ternary Alloys, V. Nickel-Chromium-Silicon System[J]. J. Inst. Metals, 1960, 88: 373 | [17] | Ghosh G. Cr-Ni-Si (Chromium-Nickel-Silicon)[M]// Non-Ferrous Metal Systems. Part 3. Springer Berlin Heidelberg, 2007: 229 | [18] | Cui C, Zhang J, Wu K, et al.Microstructure and properties of Ni-Ni3Si composites by directional solidification[J]. Physica B, 2012, 407(17): 3566 |
|
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|