Download:  PDF(2181KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The oxidation behavior of powder metallurgical Ag--Cr ~alloys ~at ~700 and 800℃ ~in ~0.1~MPa O{2} was studied. PM Ag--35Cr alloy formed complex scale including silver metal, Cr$_{2}$O$_{3}$, AgCrO$_{2}$ and internal oxidation zone of chromium. A continuous layer of Cr$_{2}$O$_{3}$ under an external layer of AgCrO$_{2}$ formed on the PM Ag--69Cr alloy. The internal oxidation of chromium was suppressed in this alloy. The oxidation of PM Ag--Cr alloys was strongly affected by the restriction to chromium diffusion due to the presence of two phases and by the relatively large size of the chromium particles, which restrained the formation of exclusive Cr$_{2}$O$_{3}$ scales which restrained the formation of exclusive Cr$_{2}$O$_{3}$ scales at the chromium contents 69\%. The appearance of pure silver on the PM Ag--35Cr alloy was a result of the stress resulting from large volume change caused by internal oxidation.
Key words:  metallic materials      powder metallurgy(PM)      oxidation      Ag-Cr alloy      
Received:  31 August 2004     
ZTFLH:  TG174  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.cjmr.org/EN/     OR     https://www.cjmr.org/EN/Y2004/V18/I4/352

1 T.B.Massalski, Binary Alloys Phase Diagrams, (ASM, USA, 1986) p.17
2 F.Gesmundo, F.Viani, Y.Niu, D.L.Douglass, Oxid. Met., 40(3/4) , 373(1993)
3 F.Gesmundo, Y.Niu, F.Viani, Oxid. Met., 43(3/4) , 379(1995)
4 F.Gesmundo, F.Viani, Y.Niu, Oxid. Met., 47(3/4) , 355(1997)
5 FU Guangyan, NIU Yan, WU Weitao, Acta Metallurgica Sinica, 34(2) , 159(1998) (付广艳,牛焱,吴维(山文)金属学报,34(2) , 159(1998) )
6 FU Guangyan, NIU Yan, WU Weitao, Acta Metallurgica Sinica, 39(3) , 297(2003) (付广艳,牛焱,吴维(山文),金属学报,39(3) , 297(2003) )
7 FU Guangyan, NIU Yan, WU Weitao, Transactions of Nonferrous Metals Society of China, 12(2) , 874(2002)
8 Y.Niu, G.Y.Fu, F.Gesmundo, Corrosion Science, 41, 1791(1999)
9 F.Gesmundo, Y.Niu, D.Oquab, C.Roos, B.Pieraggi, Oxid. Met., 49(1/2) , 115(1998)
10 FU Guangyan, NIU Yan, WU Weitao, GUAN Hengrong, Transactions of Nonferrous Metals Society of
11 China, 11(3) , 333(2001)
12 G.Y.Fu, Y.Niu, F.Gesmundo, Corrosion Science, 45, 559(2003) S.Guruswamy, S.M.Park, J.P.Hirth, R.A.Rapp, Oxid Met, 26(1/2) , 77(1986)
13 D.L.Douglass, Oxid. Met., 44(1/2) , 81(1995)
[1] MAO Jianjun, FU Tong, PAN Hucheng, TENG Changqing, ZHANG Wei, XIE Dongsheng, WU Lu. Kr Ions Irradiation Damage Behavior of AlNbMoZrB Refractory High-entropy Alloy[J]. 材料研究学报, 2023, 37(9): 641-648.
[2] SONG Lifang, YAN Jiahao, ZHANG Diankang, XUE Cheng, XIA Huiyun, NIU Yanhui. Carbon Dioxide Adsorption Capacity of Alkali-metal Cation Dopped MIL125[J]. 材料研究学报, 2023, 37(9): 649-654.
[3] ZHAO Zhengxiang, LIAO Luhai, XU Fanghong, ZHANG Wei, LI Jingyuan. Hot Deformation Behavior and Microstructue Evolution of Super Austenitic Stainless Steel 24Cr-22Ni-7Mo-0.4N[J]. 材料研究学报, 2023, 37(9): 655-667.
[4] SHAO Hongmei, CUI Yong, XU Wendi, ZHANG Wei, SHEN Xiaoyi, ZHAI Yuchun. Template-free Hydrothermal Preparation and Adsorption Capacity of Hollow Spherical AlOOH[J]. 材料研究学报, 2023, 37(9): 675-684.
[5] XING Dingqin, TU Jian, LUO Sen, ZHOU Zhiming. Effect of Different C Contents on Microstructure and Properties of VCoNi Medium-entropy Alloys[J]. 材料研究学报, 2023, 37(9): 685-696.
[6] OUYANG Kangxin, ZHOU Da, YANG Yufan, ZHANG Lei. Microstructure and Tensile Properties of Mg-Y-Er-Ni Alloy with Long Period Stacking Ordered Phases[J]. 材料研究学报, 2023, 37(9): 697-705.
[7] XU Lijun, ZHENG Ce, FENG Xiaohui, HUANG Qiuyan, LI Yingju, YANG Yuansheng. Effects of Directional Recrystallization on Microstructure and Superelastic Property of Hot-rolled Cu71Al18Mn11 Alloy[J]. 材料研究学报, 2023, 37(8): 571-580.
[8] XIONG Shiqi, LIU Enze, TAN Zheng, NING Likui, TONG Jian, ZHENG Zhi, LI Haiying. Effect of Solution Heat Treatment on Microstructure of DZ125L Superalloy with Low Segregation[J]. 材料研究学报, 2023, 37(8): 603-613.
[9] LIU Jihao, CHI Hongxiao, WU Huibin, MA Dangshen, ZHOU Jian, XU Huixia. Heat Treatment Related Microstructure Evolution and Low Hardness Issue of Spray Forming M3 High Speed Steel[J]. 材料研究学报, 2023, 37(8): 625-632.
[10] YOU Baodong, ZHU Mingwei, YANG Pengju, HE Jie. Research Progress in Preparation of Porous Metal Materials by Alloy Phase Separation[J]. 材料研究学报, 2023, 37(8): 561-570.
[11] REN Fuyan, OUYANG Erming. Photocatalytic Degradation of Tetracycline Hydrochloride by g-C3N4 Modified Bi2O3[J]. 材料研究学报, 2023, 37(8): 633-640.
[12] WANG Hao, CUI Junjun, ZHAO Mingjiu. Recrystallization and Grain Growth Behavior for Strip and Foil of Ni-based Superalloy GH3536[J]. 材料研究学报, 2023, 37(7): 535-542.
[13] LIU Mingzhu, FAN Rao, ZHANG Xiaoyu, MA Zeyuan, LIANG Chengyang, CAO Ying, GENG Shitong, LI Ling. Effect of Photoanode Film Thickness of SnO2 as Scattering Layer on the Photovoltaic Performance of Quantum Dot Dye-sensitized Solar Cells[J]. 材料研究学报, 2023, 37(7): 554-560.
[14] QIN Heyong, LI Zhentuan, ZHAO Guangpu, ZHANG Wenyun, ZHANG Xiaomin. Effect of Solution Temperature on Mechanical Properties and γ' Phase of GH4742 Superalloy[J]. 材料研究学报, 2023, 37(7): 502-510.
[15] FENG Ye, CHEN Zhiyong, JIANG Sumeng, GONG Jun, SHAN Yiyin, LIU Jianrong, WANG Qingjiang. Effect of a NiCrAlSiY Coating on Cyclic Oxidation and Room Temperature Tensile Properties of Ti65 Alloy Plate[J]. 材料研究学报, 2023, 37(7): 523-534.
No Suggested Reading articles found!