Please wait a minute...
材料研究学报  2026, Vol. 40 Issue (7): 497-506    DOI: 10.11901/1005.3093.2026.111
  研究论文 本期目录 | 过刊浏览 |
Cf/ZrB2-SiC和Cf/ZrB2-SiBCN复合材料的力学、氧化和循环烧蚀性能
付俞寒1,2, 樊俊铃3, 张伟3, 庞生洋2, 胡成龙2()
1.沈阳化工大学材料科学与工程学院 沈阳 110142
2.中国科学院金属研究所 沈阳 110016
3.中国飞机强度研究所 强度与结构完整性全国重点实验室 西安 710065
Mechanical, Oxidation and Cyclic Ablation Properties of Cf/ZrB2-SiC and Cf/ZrB2-SiBCN Composites
FU Yuhan1,2, FAN Junling3, ZHANG Wei3, PANG Shengyang2, HU Chenglong2()
1.School of Materials Science and Engineering, Shenyang University of Chemical Technology, Shenyang 110142, China
2.Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
3.National Key Laboratory of Strength and Structural Integrity, Aircraft Strength Research Institute of China, Xi'an 710065, China
引用本文:

付俞寒, 樊俊铃, 张伟, 庞生洋, 胡成龙. Cf/ZrB2-SiC和Cf/ZrB2-SiBCN复合材料的力学、氧化和循环烧蚀性能[J]. 材料研究学报, 2026, 40(7): 497-506.
Yuhan FU, Junling FAN, Wei ZHANG, Shengyang PANG, Chenglong HU. Mechanical, Oxidation and Cyclic Ablation Properties of Cf/ZrB2-SiC and Cf/ZrB2-SiBCN Composites[J]. Chinese Journal of Materials Research, 2026, 40(7): 497-506.

全文: PDF(17429 KB)   HTML
摘要: 

采用料浆浸渍-前驱体浸渍裂解联合工艺(SI-PIP)制备高密度和高ZrB2含量的Cf/ZrB2-SiC和Cf/ZrB2-SiBCN复合材料,其密度分别为2.73 g/cm3和2.70 g/cm3,ZrB2含量(体积分数)超过25%;研究了不同前驱体对其氧化和烧蚀行为的影响,结果表明在1200 ℃氧化循环9次后,Cf/ZrB2-SiBCN和Cf/ZrB2-SiC的质量损失率分别为3.69%和3.59%,而在1400 ℃氧化循环次数相同后Cf/ZrB2-SiBCN的质量损失率显著高于Cf/ZrB2-SiC,达到5.05%。其主要原因是,在较高的温度下SiBCN氧化产物中的B、N挥发。Cf/ZrB2-SiBCN复合材料分别在1800 ℃和2100 ℃经9次(单次300 s)氧乙炔循环烧蚀后,其质量损失率分别为1.29%和1.93%,显著优于Cf/ZrB2-SiC复合材料。其主要原因是,Cf/ZrB2-SiBCN更致密的结构以及其在循环烧蚀时产生的玻璃相愈合了次表面裂纹,减少了燃气冲刷产生的机械剥蚀。

关键词 : 复合材料,  超高温陶瓷,  可重复使用性能,  循环氧化,  循环烧蚀    
Abstract:

The composites Cf/ZrB2-SiC and Cf/ZrB2-SiBCN with high ZrB2 content were prepared via a combined method of slurry infiltration (SI) and precursor infiltration pyrolysis (PIP), accordingly their densities are 2.73 g/cm3 and 2.70 g/cm3 respectively, and the ZrB2 content exceeding 25% (volume fraction). The effect of different precursors on the oxidation and ablation behavior of the composites was investigated, aiming to address issues such as the low reusable temperature and insufficient understanding of ablation behavior for carbon fiber-reinforced ultra-high temperature ceramic matrix composites. The results showed that after nine oxidation cycles at 1200 °C, the mass loss rates of Cf/ZrB2-SiBCN and Cf/ZrB2-SiC were comparable, at 3.69% and 3.59%, respectively. However, after the same number of oxidation cycles at 1400 oC, the mass loss rate of Cf/ZrB2-SiBCN was significantly higher than that of Cf/ZrB2-SiC, reaching 5.05%. This is primarily attributed to the volatilization of B- and N-gaseous compounds from the oxidation products of SiBCN at higher temperatures. After nine cycles of oxyacetylene flame ablation at 1800 oC and 2100 oC for a single duration of 300 s, the mass loss rates of Cf/ZrB2-SiBCN were 1.29% and 1.93%, respectively, which are significantly lower than those of Cf/ZrB2-SiC composites. This improvement is mainly due to the higher density of Cf/ZrB2-SiBCN and the better healing ability of the glass phase formed during cyclic ablation, which reduces mechanical erosion caused by gas flow and mitigates subsurface crack propagation.

Key words: composite    ultra-high-temperature ceramics    reusability    cyclic oxidation resistance    cyclic ablation
收稿日期: 2026-01-27     
ZTFLH:  TB332  
基金资助:国家自然科学基金(52572089);国家自然科学基金(52532003)
通讯作者: 胡成龙,研究员,clhu10s@imr.ac.cn,研究方向为陶瓷基复合材料及其抗氧化
Corresponding author: HU Chenglong, Tel: (024)23979833, E-mail: clhu10s@imr.ac.cn
作者简介: 付俞寒,男,1999年生,硕士生
图1  Cf/ZrB2坯体的SEM图像
图2  Cf/ZrB2坯体的孔径分布
图3  复合材料的截面微观形貌
图4  S-ZS和S-ZSB复合材料的弯曲应力-应变曲线
图5  S-ZS和S-ZSB在不同温度下氧化的质量损失曲线
图6  S-ZS和S-ZSB在不同温度下氧化不同时间后的微观形貌
图7  S-ZS和S-ZSB在不同温度循环烧蚀后的质量损失曲线
图8  S-ZS和S-ZSB复合材料在1800 ℃循环烧蚀9次后样品表面显微形貌和EDS
图9  S-ZS和S-ZSB复合材料样品在2100 ℃循环烧蚀后的表面形貌
图10  样品在2100 ℃烧蚀后表面的三维形貌以及各烧蚀坑深度区间的比例
[1] Niu C, Wang C, Chen J B, et al. Review of the recovery system of reusable launch vehicle [J]. J. Astronaut., 2025, 46(5): 825
[1] 牛 枞, 王 宸, 陈金宝 等. 可重复使用运载火箭回收着陆装置研究进展 [J]. 宇航学报, 2025, 46(5): 825
[2] Bao W M. A review of reusable launch vehicle technology development [J]. Acta Aeronaut. Astronaut. Sin., 2023, 44(23): 629555
[2] 包为民. 可重复使用运载火箭技术发展综述 [J]. 航空学报, 2023, 44(23): 629555
doi: 10.7527/S1000-6893.2023.29555
[3] Wang J X, Zhong M L, Li J X, et al. Mitigating hypersonic heat barrier via direct cooling enhanced by leidenfrost inhibition [J]. Nat. Commun., 2025, 16(1): 6931
doi: 10.1038/s41467-025-62120-2
[4] Peters A B, Zhang D J, Chen S, et al. Materials design for hypersonics [J]. Nat. Commun., 2024, 15(1): 3328
doi: 10.1038/s41467-024-46753-3 pmid: 38637517
[5] Zhu Y H, Peng W, Xu R N, et al. Review on active thermal protection and its heat transfer for airbreathing hypersonic vehicles [J]. Chin. J. Aeronaut., 2018, 31(10): 1929
doi: 10.1016/j.cja.2018.06.011
[6] Hu P, Dong S, Cheng Y, et al. Research progress on ultra-high temperature ceramic composites [J]. J. Inorg. Mater., 2024, 39(6): 571
doi: 10.15541/jim20230609
[6] 胡 平, 董 顺, 程 源 等. 超高温陶瓷复合材料研究进展 [J]. 无机材料学报, 2024, 39(6): 571
[7] Chen Y F, Hong C Q, Hu C L, et al. Ceramic-based thermal protection materials for aerospace vehicles [J]. Adv. Ceram., 2017, 38(5): 311
[7] 陈玉峰, 洪长青, 胡成龙 等. 空天飞行器用热防护陶瓷材料 [J]. 现代技术陶瓷, 2017, 38(5): 311
[8] Tang S F, Hu C L. Design, preparation and properties of carbon fiber reinforced ultra-high temperature ceramic composites for aerospace applications: a review [J]. J. Mater. Sci. Technol., 2017, 33(2): 117
[9] Li C, Yang H L, Zou J, et al. Rapid fabrication of Cf/ZrB2-SiC composites with multifunctional properties via aqueous injection-assisted vacuum impregnation [J]. Sci. China Mater., 2026, 69: 2108
doi: 10.1007/s40843-025-3487-x
[10] Wyatt B C, Nemani S K, Hilmas G E, et al. Ultra-high temperature ceramics for extreme environments [J]. Nat. Rev. Mater., 2024, 9: 733
[11] Fahrenholtz W G, Hilmas G E. Ultra-high temperature ceramics: materials for extreme environments [J]. Scr. Mater., 2017, 129: 94
doi: 10.1016/j.scriptamat.2016.10.018
[12] Liu Y, Fu Q G, Wang B B, et al. The ablation behavior and mechanical property of C/C-SiC-ZrB2 composites fabricated by reactive melt infiltration [J]. Ceram. Int., 2017, 43(8): 6138
doi: 10.1016/j.ceramint.2017.02.008
[13] Liu Y S, Wei G X, Ma Y W, et al. Process optimization and ablation performance of Cf/ZrB2-SiC composites prepared by slurry injection combined with RMI [J]. J. Am. Ceram. Soc., 2025, 108(12): e70179
doi: 10.1111/jace.v108.12
[14] Chen B W, Ni D W, Liao C J, et al. Long-term ablation behavior and mechanisms of 2D-Cf/ZrB2-SiC composites at temperatures up to 2400 °C [J]. Corros. Sci., 2020, 177(5): 108967
doi: 10.1016/j.corsci.2020.108967
[15] Chen B W, Ni D W, Lu J, et al. Multi-cycle and long-term ablation behavior of Cf/ZrB2-SiC composites at 2500 oC [J]. Corros. Sci., 2021, 184(3): 109385
doi: 10.1016/j.corsci.2021.109385
[16] Wang R N, Zhang J P, Fei J, et al. Effect of ZrB2 on the ablation behavior of Cf/ZrB2-ZrC-SiC sharp leading edge composites by PIP and RMI [J]. Mater. Charact., 2024, 211: 113898
doi: 10.1016/j.matchar.2024.113898
[17] Marumo T, Koide N, Arai Y, et al. Characterization of carbon fiber-reinforced ultra-high temperature ceramic matrix composites fabricated via Zr-Ti alloy melt infiltration [J]. J. Eur. Ceram. Soc., 2022, 42(13): 5208
doi: 10.1016/j.jeurceramsoc.2022.06.040
[18] Zhao Z G, Li K Z, Kou G, et al. Comparative research on cyclic ablation behavior of C/C-ZrC-SiC and C/C-ZrC composites at temperatures above 2000 oC [J]. Corros. Sci., 2022, 206: 110496
doi: 10.1016/j.corsci.2022.110496
[19] Grigoriev O N, Stepanenko A V, Vinokurov V B, et al. ZrB2-SiC ceramics: residual stresses and mechanical properties [J]. J. Eur. Ceram. Soc., 2021, 41(9): 4720
doi: 10.1016/j.jeurceramsoc.2021.02.053
[20] Liu Y S, Wei G X, Ma Y W, et al. Influence of slurry and injection methods on the fabrication of Cf/ZrB2‐SiC composite via slurry injection and RMI [J]. J. Am. Ceram. Soc., 2025, 108(10): e70031
doi: 10.1111/jace.v108.10
[21] Zhang D Y, Hu P, Dong S, et al. Oxidation behavior and ablation mechanism of Cf/ZrB2-SiC composite fabricated by vibration-assisted slurry impregnation combined with low-temperature hot pressing [J]. Corros. Sci., 2019, 161: 108181
doi: 10.1016/j.corsci.2019.108181
[22] Zhao Z G, Li K Z, Li W, et al. Cyclic ablation behavior of C/C-ZrC-SiC-ZrB2 composites under oxyacetylene torch with two heat fluxes at the temperatures above 2000 oC [J]. Corros. Sci., 2021, 181: 109202
doi: 10.1016/j.corsci.2020.109202
[23] Xie J, Li K Z, Li H J, et al. Cyclic ablation behavior of C/C-ZrC-SiC composites under oxyacetylene torch [J]. Ceram. Int., 2014, 40(4): 5165
doi: 10.1016/j.ceramint.2013.10.069
[24] Hu C L, Pang S Y, Tang S F, et al. An integrated composite with a porous Cf/C-ZrB2-SiC core between two compact outer layers of Cf/C-ZrB2-SiC and Cf/C-SiC [J]. J. Eur. Ceram. Soc., 2015, 35(3): 1113
doi: 10.1016/j.jeurceramsoc.2014.10.005
[25] Ding Q, Ni D W, Wang Z, et al. Effect of interphase on mechanical properties and microstructures of 3D Cf/SiBCN composites at elevated temperatures [J]. J. Am. Ceram. Soc., 2019, 102(6): 3630
doi: 10.1111/jace.16202
[26] Ji S Y, Liang B, Yang B, et al. Long-term oxidation behaviors and strength retention properties of self-healing SiCf/SiC-SiBCN composites [J]. J. Eur. Ceram. Soc., 2023, 43(5): 1843
doi: 10.1016/j.jeurceramsoc.2022.12.009
[27] Gao Q, Hu P, Xun L C, et al. A scalable method allows for the rapid fabrication of C/SiC composites with excellent mechanical properties and ablation resistance [J]. J. Adv. Ceram., 2025, 14(10): 9221162
doi: 10.26599/JAC.2025.9221162
[28] Lee S H, Weinmann M, Aldinger F. Fabrication of fiber‐reinforced ceramic composites by the modified slurry infiltration technique [J]. J. Am. Ceram. Soc., 2007, 90(8): 2657
doi: 10.1111/jace.2007.90.issue-8
[29] Zhang C, Hu P, Xun L C, et al. A universal strategy towards the fabrication of ultra-high temperature ceramic matrix composites with outstanding mechanical properties and ablation resistance [J]. Compos. Pt. B-Eng., 2024, 280: 111485
doi: 10.1016/j.compositesb.2024.111485
[30] Jiang L Y, Tang S F, Zhang Y, et al. Preparation and oxidation behaviors of C/SiC-BN composites [J]. J. Inorg. Mater., 2024, 39(7): 779
doi: 10.15541/jim20230583
[30] 姜灵毅, 汤素芳, 张 悦 等. C/SiC-BN复合材料的制备及氧化行为 [J]. 无机材料学报, 2024, 39(7): 779
[1] 李嘉文, 于巍, 王鹏, 庄印, 白玉, 郝海. 铝基互穿相多孔复合材料的制备及其力学性能[J]. 材料研究学报, 2026, 40(8): 605-612.
[2] 王俊, 刘雯, 籍伟花, 苗洋, 王一杰, 宗振昊, 马浩铭, 周玲玲. NiFe-LDH/Co, La-CeO2 催化剂的制备及其性能[J]. 材料研究学报, 2026, 40(7): 507-518.
[3] 赵俊杰, 明孝, 刘倩倩, 曾小平, 王大威, 王玮, 吴江渝. 碳纤维/二硫化钼改性纤维素复合气凝胶的制备及其吸声性能[J]. 材料研究学报, 2026, 40(7): 528-534.
[4] 王雨晴, 王金贺, 李可馨, 付华萌, 张海峰. W/TiZrVAl高熵合金复合材料制备和性能[J]. 材料研究学报, 2026, 40(7): 553-560.
[5] 姜兴国, 沈文卓, 杨涛, 张佳利, 钟民, 曹贺, 郭守武. 还原氧化石墨烯铜基复合材料的耐腐蚀性能及其机理[J]. 材料研究学报, 2026, 40(6): 450-456.
[6] 于瀚博, 胡妍, 徐婷婷, 张一文, 张弛, 谭杰文, 李永翔, 王晗. Bi4O5I2/Bi7O9I3 异质结光催化剂对水中环丙沙星的降解性能[J]. 材料研究学报, 2026, 40(5): 321-332.
[7] 刘丹阳, 景苗苗, 赵强, 王俊丽, 贾治芳, 李作鹏, 王科伟, 郭永. Cu2O/N,S-BiOBr复合光催化剂的制备及其降解性能[J]. 材料研究学报, 2026, 40(5): 333-342.
[8] 屈梦原, 游康伟, 谢丽燕, 王雅馨, 罗志珊, 黄建辉. Bi/Bi2O2CO3 等离子体复合材料的合成及其光催化性能[J]. 材料研究学报, 2026, 40(5): 343-351.
[9] 李倩, 史桂梅. 核壳结构Ni-TiN@CN纳米复合材料的吸波性能[J]. 材料研究学报, 2026, 40(5): 372-384.
[10] 黄实哈, 董星龙, 裴雷振, 张兴国. 核/壳结构FeSiBCuNbZr@SiO2 非晶复合材料的制备及其微波吸收性能[J]. 材料研究学报, 2026, 40(4): 254-262.
[11] 胡道春, 王蕾, 见小琪, 陈明和, 周颖. 使用Ni中间层SPS扩散连接金刚石/铜复合材料界面的导热性能[J]. 材料研究学报, 2026, 40(2): 152-160.
[12] 朱皓文, 隋国鑫, 刘冬艳. 聚丙烯和烯烃嵌段共聚物半导电屏蔽层的性能[J]. 材料研究学报, 2026, 40(1): 23-30.
[13] 刘金玲, 张艳, 戚栋明, 虞一浩. 三明治结构复合薄膜的制备及其阻燃与电磁屏蔽性能研究[J]. 材料研究学报, 2025, 39(9): 650-660.
[14] 颉芳霞, 吴光庆, 张世文, 卢泽异, 牟彦铭, 何雪明. 7075-TiB2 复合材料的制备和性能[J]. 材料研究学报, 2025, 39(9): 683-693.
[15] 王炳林, 柴一峰, 谭圣霞, 郭升伟, 姜如, 朱中华, 张禹涛, 黄桂芳, 黄维清. g-C3N4/CdS S型异质结复合光催化材料的制备及其性能[J]. 材料研究学报, 2025, 39(9): 712-720.