Abstract The geopolymer composites of coal gangue-slag were prepared with sodium hydroxide (NH) and sodium silicate (NS) as activator. The effect of slag content and NH modules on the fluidity of cement pastes and compressive strength of alkali-activated coal gangue-slag (AACGS) cementitious materials was investigated. The property of the prepared cementitious materials and the relevant cementation mechanism were investigated by means of mechanical test, XRD, FT-IR, MAS NMR and SEM-EDS. Results show that the slag content has significant effect on the pastes fluidity and compressive strength, while the NH module only has significant effect on the compressive strength of AACGS cementitious materials. Higher early strength may be produced for AACGS materials, for instance, when the slag content exceeds 20%, the 28 d strength is also higher than that of P. O42.5 pure cement. With the increase of slag content, the higher polymerization degree emerged for the silicate structure in the hydration products, which is consistent with the measured results of compressive strength. Since that Ca2+ has a stronger drive adsorption force than Na+, therewith the increase of slag content from 0 to 50% may result in denser matrix, of which the C-(A)-S-H in the microstructure has higher Ca/Si ratio but lower Al/Si ratio. The disordered network structure of AACGS, which consists of C-A-S-H gels and C-S-H gels and N-A-S-H gels, has good compatibility.
|
Received: 29 May 2018
|
Fund: Supported by National Natural Science Foundation of China (No. 51578539), Beijing Natural Science Foundation Projects (No. 8164061), Open Research Project of State Key Laboratory of Coal Resources and Safe Mining, China University of Mining and Technology (No. SKLCRSM16KFD07) |
[1] | Wang J, Wu X L, Wang J X, et al.Hydrothermal synthesis and characterization of alkali-activated slag-fly ash-metakaolin cementitious materials[J]. Micropor. Mesopor. Mater., 2012, 155: 186 | [2] | Li Y J, Yan X P, Zhang X, et al.Experimental research on seismic behavior of reinforced concrete column composed of coal gangue aggregate[J]. J. Chin. Coal Soc., 2013, 38: 1006(李永靖, 闫宣澎, 张旭等. 煤矸石骨料钢筋混凝土柱的抗震性能试验研究[J]. 煤炭学报, 2013, 38: 1006) | [3] | Guo W, Li D X, Chen J H, et al.Structure and pozzolanic activity of calcined coal gangue during the process of mechanical activation[J]. J. Wuhan Univ. Technol.-Mater. Sci. Ed., 2009, 24: 326 | [4] | Yi C, Ma H Q, Zhu H G, et al.Study on chloride binding capability of coal gangue based cementitious materials[J]. Constr. Build. Mater., 2018, 167: 649 | [5] | Yi C, Ma H Q, Zhu H G, et al.Investigation on anti-carbonation performance of coal gangue coarse aggregate concrete[J]. J. Build. Mater., 2017, 20: 787(易成, 马宏强, 朱红光等. 煤矸石粗集料混凝土抗碳化性能研究[J]. 建筑材料学报, 2017, 20: 787) | [6] | Ben Haha M, Le Saout G, Winnefeld F, et al.Influence of activator type on hydration kinetics, hydrate assemblage and microstructural development of alkali activated blast-furnace slags[J]. Cem. Concr. Res., 2011, 41: 301 | [7] | Puertas F, Palacios M, Manzano H, et al.A model for the C-A-S-H gel formed in alkali-activated slag cements[J]. J. Eur. Ceram. Soc., 2011, 31: 2043 | [8] | Cui X W, Ni W, Ren C.Hydration mechanism of all solid waste cementitious materials based on steel slag and blast furnace slag[J]. Chin. J. Mater. Res., 2017, 31: 687(崔孝炜, 倪文, 任超. 钢渣矿渣基全固废胶凝材料的水化反应机理[J]. 材料研究学报, 2017, 31: 687) | [9] | Pacheco-Torgal F, Castro-Gomes J, Jalali S.Alkali-activated binders: a review: Part 1. Historical background, terminology, reaction mechanisms and hydration products[J]. Constr. Build. Mater., 2008, 22: 1305 | [10] | Zuda L, Drchalová J, Rovnaník P, et al.Alkali-activated aluminosilicate composite with heat-resistant lightweight aggregates exposed to high temperatures: mechanical and water transport properties[J]. Cem. Concr. Comp., 2010, 32: 157 | [11] | Huang G D, Ji Y S, Li J, et al.Improving strength of calcinated coal gangue geopolymer mortars via increasing calcium content[J]. Constr. Build. Mater., 2018, 166: 760 | [12] | T?nzer R, Buchwald A, Stephan D.Effect of slag chemistry on the hydration of alkali-activated blast-furnace slag[J]. Mater. Struct., 2015, 48: 629 | [13] | Zhang C S, Xue J P, Fang L M.Mechanical properties and microstructures of alkali activated burned coal gangue cementitious material[J]. J. Chin. Ceram. Soc., 2004, 32: 1276(张长森, 薛建平, 房利梅. 碱激发烧煤矸石胶凝材料的力学性能和微观结构[J]. 硅酸盐学报, 2004, 32: 1276) | [14] | Provis J L, Myers R J, White C E, et al.X-ray microtomography shows pore structure and tortuosity in alkali-activated binders[J]. Cem. Concr. Res., 2012, 42: 855 | [15] | Phair J W, van Deventer J S J. Effect of the silicate activator PH on the microstructural characteristics of waste-based geopolymers[J]. Int. J. Miner. Process., 2002, 66: 121 | [16] | Heikal M, Nassar M Y, El-Sayed G, et al.Physico-chemical, mechanical, microstructure and durability characteristics of alkali activated Egyptian slag[J]. Constr. Build. Mater., 2014, 69: 60 | [17] | Ismail I, Bernal S A, Provis J L, et al.Modification of phase evolution in alkali-activated blast furnace slag by the incorporation of fly ash[J]. Cem. Concr. Comp., 2014, 45: 125 | [18] | Lancellotti I, Catauro M, Ponzoni C, et al.Inorganic polymers from alkali activation of metakaolin: effect of setting and curing on structure[J]. J. Solid State Chem., 2013, 200: 341 | [19] | Ye H L, Radlińska A.Shrinkage mechanisms of alkali-activated slag[J]. Cem. Concr. Res., 2016, 88: 126 | [20] | Melo Neto A A, Cincotto M A, Repette W. Drying and autogenous shrinkage of pastes and mortars with activated slag cement[J]. Cem. Concr. Res., 2008, 38: 565 | [21] | Cartwright C, Rajabipour F, Radlińska A.Shrinkage characteristics of alkali-activated slag cements[J]. J. Mater. Civil. Eng., 2015, 27: B4014007 | [22] | Garcia-Lodeiro I, Palomo A, Fernández-Jiménez A, et al.Compatibility studies between N-A-S-H and C-A-S-H gels. Study in the ternary diagram Na2O-CaO-Al2O3-SiO2-H2O[J]. Cem. Concr. Res., 2011, 41: 923 | [23] | Guo X L, Shi H S, Xia M.Effect of different calcium resouces on reaction mechanism of geopolymer[J]. Chin. J. Mater. Res., 2016, 30: 348(郭晓潞, 施惠生, 夏明. 不同钙源对地聚合物反应机制的影响研究[J]. 材料研究学报, 2016, 30: 348) | [24] | Weng L, Sagoe-Crentsil K.Dissolution processes, hydrolysis and condensation reactions during geopolymer synthesis: Part I—Low Si/Al ratio systems[J]. J. Mater. Sci., 2007, 42: 2997 | [25] | Zhang C S, Fang L M.Hardening mechanisms of alkali activated burned gangue cementitious material[J]. Mater. Sci. Technol., 2004, 12: 597(张长森, 房利梅. 碱激发烧煤矸石胶凝材料的硬化机理研究[J]. 材料科学与工艺, 2004, 12: 597) |
|
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|