Please wait a minute...
Chin J Mater Res  2008, Vol. 22 Issue (3): 287-290    DOI:
Research Articles Current Issue | Archive | Adv Search |
The hardess degradation of naocomposite Ti-Si-N coatings induced by oxygen impurity and its mechanisms
;;;
西安交通大学
Cite this article: 

;. The hardess degradation of naocomposite Ti-Si-N coatings induced by oxygen impurity and its mechanisms. Chin J Mater Res, 2008, 22(3): 287-290.

Download:  PDF(839KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  There has been a wide attention in nanocomposite coatings with interface phases because of their superhardness, but the limitation hardness that this kind of materials can achieve was still an argued question by many researchers. In this paper, we observe the limitation hardness of nanocomposite coatings is very sensitive to microstructure of interface. It is shown that a dependent relation between hardness and oxygen impurity content of coatings resulted from our experiments. Based on an atomic model analysis, the decreasing of hardness caused by a small amount of oxygen impurities can be explained by oxygen atoms induce weakening of the Si3N4 interface which acts as a “glue” between the TiN nanocrystals. Further, we conclude that density of oxygen atoms around grain boundary is a dominant factor on hardness degradation of the films
Key words:       
Received:  28 June 2007     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.cjmr.org/EN/     OR     https://www.cjmr.org/EN/Y2008/V22/I3/287

1 MA Dayan,MA Shengli,XU Kewei,S.Veprek,A study on thermal stability of nano-structure Ti-Si-N coatings at elevated temperature,Chinese Journal of Materials Re- search,18(6),617(2004) (马大衍,马胜利,徐可为,S.Veprek,纳米Ti-Si-N薄膜的高温热稳定性研究,材料研究学报,18(6),617(2004))
2 S.Veprek,P.Nesladek,A.Niederhofer,Search for super- hard materials:nanocrystalline composites with hard- ness exceeding 50 GPa,Nanostructured Materials,10(5), 679(1998)
3 J.Haines,J.M.Léger,G.Bocquillon,Synthesis and design of superhard materials,Annu.Rev.Mater.Res.,31(1), 25(2001)
4 Wang Y.M.,Chen M.W.,Zhou F.H.,Ma E.,High ten- sile ductility in a nanostructured metal,Nature,419, 912(2002)
5 S.Li,Y.Shi,H.Peng,Ti-Si-N films prepared by plasma- enhanced chemical vapour deposition,Plasma Chemistry and Plasma Processing,12(3),287(1992)
6 J.Patscheider,Nanocomposite hard coatings for wear pro- tection,MRS Bull.,28(3),180(2003)
7 Fanghua MEI,Nan SHAO,Xiaoping HU,Geyang LI, Mingyuan GU,Microstructure and mechanical properties of reactively sputtered Ti-Si-N nanocomposite films,Ma- terials Letters,59,2442(2005)
8 W.J.Meng,X.D.Zhang,B.Shi,R.C.Tittsworth,L.E.Rehn, P.M.Baldo,Microstructure and mechanical properties of Ti-Si-N coatings,J.Mater.Res.,17,2628(2002)
9 S.H.Kim,J.K.Kim,K.H.Kim,Influence of deposition con- ditions on the microstructure and mechanical properties of Ti-Si-N films by DC reactive magnetron sputtering,Thin Solid Films,420-421,360(2002)
10 P.Vaz,L.Rebouta,Ph.Godeau,T.Girardeau,J.Pacaud, J.P.Riviere,A.Traverse,Structural transitions in hard Si- based TiN coatings:the effect of bias voltage and temper- ature,Surf.Coat.Technol.,146-144,274(2001)
11 S.A.Barnet,A.Madan,Superhard superlattices,Phys. World,11,45(1998)
12 X.Chu,S.A.Barnett,M.S.Wong,W.D.Sproul,Re- active unbalanced magnetron sputter deposition of polycrystalline TiN/NbN superlattice coatings,Surf. Coat.Technol.,57,13(1993)
13 X.T.Zeng,S.Mridha,U.Chai,Properties of unbalanced magnetron sputtered TiN/NbN multilayer coatings,Jour- nal of Materials Processing Technology,89-90,528(1999)
14 S.Veprek,A.Niederhofer,K.Moto,T.Bolom,H.-D. Mnnling,P.Nesladek,G.Dollinger and A.Bergmaier, Composition,nanostructure and origin of the ultrahard- hess in nc-TiN/α-Si_3N_4/a-and nc-TiSi_2 nanocomposites with Hv=80 to 105 GPa,Surf.Coat.Technol.,133-134, 152(2000)]
[1] Xunzeng HUANG,Yitao YANG. High Temperature Oxidation Performance of a Nb and Ti Stabilized 430 Ferritic Stainless Steel[J]. 材料研究学报, 2014, 28(9): 641-648.
[2] . [J]. 材料研究学报, 2006, 20(4): 348-353.
[3] . [J]. 材料研究学报, 2006, 20(2): 191-196.
[4] . [J]. 材料研究学报, 2006, 20(3): 322-326.
[5] . [J]. 材料研究学报, 2002, 16(4): 425-428.
[6] Tingting LI,Yong HU,Xiaoming CUI,Zhijie YAN. Micro-hardness and Shear Bands of Zr-Al-Cu-Ni-Ag Bulk Metallic Glass Composites[J]. 材料研究学报, 2014, 28(10): 730-736.
[7] . [J]. 材料研究学报, 2005, 19(6): 651-656.
[8] SHAO Guoxiang CHEN Weixiao (Fudan University). THE CHEMICAL REACTIONS OCCURRING DURING MELT MIXING OF PBT AND LDPE MODIFIED BY GRAFTING OF DIBUTYLMALEATE[J]. 材料研究学报, 1991, 5(6): 518-523.
[9] ZHOU Benlian (Institute of Metal Research;Academia Sinica)(International Centre Materials Physics;Academia Sinica). SOME PROGRESS IN THE STUDY OF ADVANCED COMPOSITE MATERIALS[J]. 材料研究学报, 1991, 5(6): 524-532.
[10] . [J]. 材料研究学报, 2003, 17(4): 433-438.
[11] LI Pengyu, LIU Zitong, KANG Shumei, CHEN Shanshan. Effect of Plasma Treatment on Performance of Polybutylene Adipate Coating on Biomedical AZ31 Mg-alloy[J]. 材料研究学报, 2023, 37(4): 271-280.
[12] HAO Jian, LIU Fang, YANG Shulin, YAO Xiaoyu, SUN Wenru. Effect of Melting Rate on Structure and Inclusions of GH4169G Alloy Ingot Fabricated by Argon Protected Electroslag Melting[J]. 材料研究学报, 2022, 36(11): 811-820.
[13] CHEN Yizi, ZHANG Chengshuang, CHEN Ping. Surface Graft Modification of Domestic PBO Fiber by Atmospheric Air Plasma[J]. 材料研究学报, 2021, 35(9): 641-650.
[14] Xusheng WANG,Guirong YANG,Wenming SONG,Jian LI,Ying MA,Yuan HAO. Microstructure and Wear Resistance of Composite Coatings Ni-Co/WC+G[J]. 材料研究学报, 2017, 31(3): 195-202.
[15] . [J]. 材料研究学报, 2001, 15(3): 303-307.