TENSILE PROPERTIES AND MICROSTRUCTURE OF AGED Ti-6Al-4V ALLOY SUBJECTED TO CYCLIC TEMPERATURE FIELD |
GENG Hongbin; HE Shiyu; LEI Tingquan (Harbin Institute of Technology) |
|
Cite this article:
GENG Hongbin; HE Shiyu; LEI Tingquan (Harbin Institute of Technology). TENSILE PROPERTIES AND MICROSTRUCTURE OF AGED Ti-6Al-4V ALLOY SUBJECTED TO CYCLIC TEMPERATURE FIELD. Chin J Mater Res, 1997, 11(4): 415-418.
|
Abstract The thermal cycling tests between 77 and 623K were performed on the aged Ti-6Al-4V alloy and the tensile properties before and after thermal cycling were evaluated. The results show that the strength of the near-peak-aged alloy decreases and that of the o
|
Received: 25 August 1997
|
1吴运学宇航材料及工艺4,62(1992) 2盛磊。宇航材料及工艺 4,27(1992) 3金峰.宇航材料及工艺.4,24(1991) 4邱惠中 宇航材料及工艺4,1(1991) 5李承受.宇航学报.1,7(1992) 6S.M.Russ,Metall.Trans.A.21(66),1595(1990) 7Haiime Ikuno,Shin-ichi Towata,J.Japan Inst.Metals,53(3),327(1989) 8E.A.鲍利索娃著.陈石卿译.铁合金金相学(北京,国防工业出版社,1980)p.8 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|