SiCf/SiC复合材料用B-N-Si新型界面相的高通量制备与性能研究
雷一明, 石金瑜, 吕熙睿, 张洁, 王京阳

High-throughput Screening of a Novel B-N-Si Interphase for Continuous SiC Fiber Reinforced SiC Ceramic Matrix Composites
LEI Yiming, SHI Jinyu, LV Xirui, ZHANG Jie, WANG Jingyang
图6 Si含量为7.57%、8.22%、11.76%和17.44%的B-N-Si薄膜在900 ℃、90%H2O-10%O2条件下氧化后的表面形貌
Fig.6 Surface morphologies of B-N-Si coatings with Si content of 7.57% (a), 8.22% (b), 11.76% (c) and 17.44% (d) after oxidation in 90%H2O-10%O2 at 900 oC