临界退火工艺对500 MPa级风电用钢焊接接头断裂韧性的优化 |
| 高崇, 熊理晞, 陈子豪, 梁治智, 麻衡, 何康, 何金珊, 庞建超, 张哲峰 |
|
Optimization of Fracture Toughness of Welded Joints of Q500 Steel Plates by Intercritical Annealing |
| GAO Chong, XIONG Lixi, CHEN Zihao, LIANG Zhizhi, MA Heng, HE Kang, HE Jinshan, PANG Jianchao, ZHANG Zhefeng |
| 图9 各CTOD试样的预制疲劳裂纹区、裂纹扩展区和剪切唇的微观形貌 |