Bi4O5I2/Bi7O9I3 异质结光催化剂对水中环丙沙星的降解性能
于瀚博, 胡妍, 徐婷婷, 张一文, 张弛, 谭杰文, 李永翔, 王晗

Degradation Performance of Heterojunction Photocatalyst Bi4O5I2/Bi7O9I3 for Ciprofloxacin Solution
YU Hanbo, HU Yan, XU Tingting, ZHANG Yiwen, ZHANG Chi, TAN Jiewen, LI Yongxiang, WANG Han
表1 铋系光催化剂降解CIP性能的对比
Table 1 Comparison of the degradation effect of CIP by bismuth-based photocatalysts
PhotocatalystConcentration / mg·L-1Dosage / g·L-1Time / minRemoval / %Light sourceReference
Bi-Bi2WO6/BiOI2018096.0300 W XL (λ ≥ 420 nm)[23]
BiOI/sulfated TiO22016085.6150 W LED (λ = 420 nm)[24]
Bi4O5I2/g-C3N4250.59066.8300 W XL (λ ≥ 420 nm)[25]
Gd-Bi4O5I2100.412094.5300 W XL (λ = 420 nm)[26]
UiO-66-NH2/Bi7O9I3100.59096.9300 W XL (λ ≥ 420 nm)[27]
Bi7O9I3-erythritol200.346076.8300 W XL (Full spectra)[28]
CuS/Bi7O9I3200.66095.21 kW XL (λ ≥ 420 nm)[29]
Bi4O5I2/Bi7O9I3200.530100.0300 W XL (λ ≥ 420 nm)This study