GH4065A合金铸态的组织和元素偏析及其均匀化 |
| 赵书伟, 孙文儒, 吕文龙, 张伟红, 邱克强 |
|
Elements Segregation and Microstructure Homogenization of Cast GH4065A Superalloy |
| ZHAO Shuwei, SUN Wenru, LV Wenlong, ZHANG Weihong, QIU Keqiang |
| 图13 GH4065A合金在不同温度保温1 h后和两阶段均匀化制度处理后的金相形貌 |
| Fig.13 OM microstructures of GH4065A alloy after holding at temperatures of 1070 oC (a), 1080 oC (b), 1130 oC (c), 1170 oC(d) and 1190 oC (e) for 1 h and after treated at 1110 oC × 20 h + 1160 oC × 20 h (f) |
|