回火时间对2300 MPa屈服强度应变-时效中锰钢组织性能的影响 |
| 刘炫业, 刘屹, 汪净, 肖大恒, 贾蕴航, 李春雨, 李云杰, 袁国, 王国栋 |
|
Influence of Tempering Duration on Microstructural Evolution and Mechanical Behavior of Strain-aged Medium-manganese Steel with 2300 MPa Yield Strength |
| LIU Xuanye, LIU Yi, WANG Jing, XIAO Daheng, JIA Yunhang, LI Chunyu, LI Yunjie, YUAN Guo, WANG Guodong |
| 图3 不同回火时间试样的组织 |
| Fig.3 Microstructure of sample of different tempering time (a) initial sample; (b) 20 min; (c) 1 h; (d) 2 h; (e) 1 h |
|