紧密排布结构大模组铸造DD5单晶高温合金的凝固组织
刘家宝, 高雪峰, 张皓宇, 王亮, 王延辉, 乐献刚, 孟杰, 李金国, 周亦胄

Microstructure of DD5 Single Crystal High-temperature Alloy Prepared via Rapid Solidification Process by Using a Large Module with Dense Array of Seed Crystals
LIU Jiabao, GAO Xuefeng, ZHANG Haoyu, WANG Liang, WANG Yanhui, YUE Xiangang, MENG Jie, LI Jinguo, ZHOU Yizhou
表2 模拟中使用的初始条件和边界条件
Table 2 Model parameters for solidification modelling
Initial conditionParameter
Melting temperature of DD5 superalloy1520 oC
Temperature of mold1520 oC
Temperature of chill plate40 oC
Boundary condition
Heater temperature1470 oC/1520 oC
Emissivity (ɛ)0.8
Cooler temperature25 oC
Interface heat transfer coefficients
Alloy melt and ceramic shell mold500 W / (m2·K)
Alloy melt and water-cooled chill plate2000 W / (m2·K)
Ceramic shell mold and water-cooled chill plate1000 W / (m2·K)