面向等离子体第一壁W-Y2O3 复合材料的力学性能
陈昱溟, 朱晓勇, 谭晓月, 刘家琴, 吴玉程

Mechanical Properties of W-Y2O3 Composites as Candidate of the First Wall Material Faced Plasma
CHEN Yuming, ZHU Xiaoyong, TAN Xiaoyue, LIU Jiaqin, WU Yucheng
表1 纯W和W-Y2O3复合材料的抗拉强度和对应的伸长率
Table 1 Tensile strength and the corresponding percentage elongation of pure W and W-Y2O3
T / oCPure WW-Y2O3
σs / MPaεp / %σs / MPaεp / %
300702.52.4458.06.1
400546.911.1436.521.3
500478.310.0376.730.3
600426.19.4338.332.7
800387.05.5278.230.7