面向等离子体第一壁W-Y2O3 复合材料的力学性能 |
陈昱溟, 朱晓勇, 谭晓月, 刘家琴, 吴玉程 |
Mechanical Properties of W-Y2O3 Composites as Candidate of the First Wall Material Faced Plasma |
CHEN Yuming, ZHU Xiaoyong, TAN Xiaoyue, LIU Jiaqin, WU Yucheng |
图7 W-Y2O3复合材料在不同温度拉伸的断口形貌 |
Fig.7 Fracture morphologies of W-Y2O3 composite after tensile test at RT (a), 200 oC (b), 300 oC (c), 400 oC (d), 500 oC (e), 600 oC (f), and 800 oC (g) |
![]() |