无氟化学溶液法制备YBCO超导焊料的高温生长工艺研究 |
| 韩磊磊, 王文涛, 吴赟, 陈嘉俊, 赵勇 |
|
High Temperature Growth Process of YBCO Superconducting Solder by Fluorine-free Chemical Solution Method |
| HAN Leilei, WANG Wentao, WU Yun, CHEN Jiajun, ZHAO Yong |
| 图9 YBCO多晶膜在820 ℃烧结30 min制备的单晶膜带材和原带材的V-I曲线 |
| Fig.9 V-I curves of the original tape and the tape with single crystal film prepared by sintering YBCO polycrystalline film at 820 oC for 30 min |
|