碱刻蚀埃洛石纳米管装载2-巯基苯并噻唑自修复涂层的制备和性能
包继华, 武鹏, 张浩然, 褚贵文, 宋立英, 蒋全通, 麻福斌

Self-healing Performance of a Novel Coating Composed of Polydimethylsiloxane Matrix and Surface Modified Halloysite Nanotubes Filler
BAO Jihua, WU Peng, ZHANG Haoran, CHU Guiwen, SONG Liying, JIANG Quantong, MA Fubin
图10 浸入3.5% NaCl溶液中的含CP-HNTs-MBT涂层上的划痕在0 d和8 d后的SEM图像和EDS数据
Fig.10 SEM image and EDS data of coating scratch area with CP-HNTs-MBT immersed in 3.5% NaCl solution for 0 d (a) and 8 d (b)