碱刻蚀埃洛石纳米管装载2-巯基苯并噻唑自修复涂层的制备和性能 |
包继华, 武鹏, 张浩然, 褚贵文, 宋立英, 蒋全通, 麻福斌 |
Self-healing Performance of a Novel Coating Composed of Polydimethylsiloxane Matrix and Surface Modified Halloysite Nanotubes Filler |
BAO Jihua, WU Peng, ZHANG Haoran, CHU Guiwen, SONG Liying, JIANG Quantong, MA Fubin |
图9 CP-HNTs-MBT划痕涂层在3.5% NaCl溶液中浸泡0 d、4 d、6 d和8 d后的SKP电位分布 |
Fig.9 SKP test of coating scratch area with CP-HNTs-MBT immersed in 3.5% NaCl solution for 0 d (a), 4 d (b), 6 d (c), 8 d (d) |
![]() |