碱刻蚀埃洛石纳米管装载2-巯基苯并噻唑自修复涂层的制备和性能
包继华, 武鹏, 张浩然, 褚贵文, 宋立英, 蒋全通, 麻福斌

Self-healing Performance of a Novel Coating Composed of Polydimethylsiloxane Matrix and Surface Modified Halloysite Nanotubes Filler
BAO Jihua, WU Peng, ZHANG Haoran, CHU Guiwen, SONG Liying, JIANG Quantong, MA Fubin
图7 在3.5% NaCl溶液中浸泡0、8、16、24和30 d后CP-HNTs-MBT涂层和空白涂层上划痕的Nyquist和Bode图
Fig.7 After immersing in a 3.5% NaCl solution for 0, 8, 16, 24, and 30 d, Nyquist (a, c) and Bode (b, d) plots of scratches on copper coated with CP-HNTs-MBT (a, b) and blank-coated surfaces (c, d)