在模拟太阳光下溶剂热时长对MIL-88A(Fe)活化过一硫酸盐降解罗丹明B催化性能的影响 |
任学昌, 安菊, 付宁, 姚小庆, 杨镇瑜, 陈泓锦 |
Degradation of RhB by MIL-88A (Fe) Activated Persulfate under Simulated Sunlight: Effect of Solvent-thermal Duration on Catalytic Performance |
REN Xuechang, AN Ju, FU Ning, YAO Xiaoqing, YANG Zhenyu, CHEN Hongjin |
图6 不同溶剂热时长MIL-88A(Fe)的UV-Vis DRS谱 |
Fig.6 UV-Vis DRS spectra (a, b) and band gap width representation (c, d) of MIL-88A(Fe) with different solvent thermal durations |
![]() |