热处理对一种 γʹ 沉淀强化钴基高温合金拉伸性能的影响
张慧芳, 吴浩, 肖传民, 李奇, 谢君, 李金国, 王振江, 于金江

Effect of Heat Treatment on Microstructure and Tensile Properties of a Typical γʹ-strengthened Co-based Superalloy
ZHANG Huifang, WU Hao, XIAO Chuanmin, LI Qi, XIE Jun, LI Jinguo, WANG Zhenjiang, YU Jinjiang
图7 合金的铸态组织、1120 ℃/3 h固溶处理后的组织以及1120 ℃/6 h固溶处理后的组织
Fig.7 SEM micrographs of as-cast alloy (a), the heat-treated microstructure after solutioned at 1120 oC for 3 h (b) and the heat-treated microstructure after solutioned at 1120 oC for 6 h (c)