热等静压态镍基高温合金的高温氧化 |
| 钟伟杰, 焦东玲, 刘仲武, 刘娜, 许文勇, 李周, 张国庆 |
|
High Temperature Oxidation of a HIPed Nickel-based Superalloy |
| ZHONG Weijie, JIAO Dongling, LIU Zhongwu, LIU Na, XU Wenyong, LI Zhou, ZHANG Guoqing |
| 图7 热等静压态高温合金在950 ℃氧化不同时间后表面氧化层元素的分布 (a) 0.5 h (b) 24 h (c) 500 h |
| Fig.7 Element distribution of surface oxide layer of as-HIPed superalloy oxidized at 950 oC |
|