奥氏体耐热钢Sanicro25的高温压痕蠕变行为
张浩杰, 林通, 赵杰, 曹铁山, 程从前

High-temperature Indentation Creep Behavior of an Austenitic Heat-resistant Steel Sanicro25
ZHANG Haojie, LIN Tong, ZHAO Jie, CAO Tieshan, CHENG Congqian
图3 Sanicro25钢在1073 K的压痕蠕变曲线
Fig.3 Sanicro25 indentation creep curves at 1073 K (a) repeated three measurement curves at different stresses at 1073 K, (b) indentation creep rate-depth