热等静压SLM Ti-6Al-4V合金的缺口敏感性
臧涛, 杨朋飞, 赵元, 高英, 鄂世举, 刘洋, 齐山贺, 张烨, 张嘉振

Effect of Hot Isostatic Pressing on Notch Sensitivity of Ti-6Al-4V Ti-alloy Prepared by Selective Laser Melting
ZANG Tao, YANG Pengfei, ZHAO Yuan, GAO Ying, E Shiju, LIU Yang, QI Shanhe, ZHANG Ye, ZHANG Jiazhen
表2 不同状态Ti-6Al-4V合金的静力拉伸力学性能
Table 2 Tensile mechanical properties of Ti-6Al-4V alloy under different processing conditions
MaterialModulus / GPaStrength / MPaElongation / %
Wrought115 ± 3.6886 ± 1719 ± 2.4
HIP-X121 ± 6.31015 ± 8.718 ± 1.7
HIP-Z117 ± 8.51022 ± 5.716 ± 2.5