1200 MPa级海洋平台用无碳化物贝氏体中锰钢腐蚀行为 |
李炎阳, 于驰, 赵伟, 高秀华, 杜林秀 |
Corrosion Behavior of 1200 MPa Class Carbide-free Bainite Medium Manganese Steel for Offshore Platform |
LI Yanyang, YU Chi, ZHAO Wei, GAO Xiuhua, DU Linxiu |
图5 不同腐蚀周期下实验钢腐蚀膜层部分宏观形貌 |
Fig.5 Macroscopic morphology of corrosion film on experimental steels under different corrosion cycles (a~c) macro morphology after corrosion for 72 h, 360 h and 576 h of 1# sample; (d~f) macro morphology after orrosion for 72 h, 360 h and 576 h of 2# sample; (g~i) macro morphology after orrosion for 72 h、360 h和576 h of 3# sample |
![]() |