增材制造高温合金在不同温度下的拉伸性能与变形机制 |
王娜, 李文彬, 庞建超, 陈立佳, 高崇, 邹成路, 张辉, 李守新, 张哲峰 |
Tensile Properties and Deformation Mechanism of Additive Manufacturing Superalloy at Different Temperatures |
WANG Na, LI Wenbin, PANG Jianchao, CHEN Lijia, GAO Chong, ZOU Chenglu, ZHANG Hui, LI Shouxin, ZHANG Zhefeng |
图4 SLM GH4169合金不同温度下的拉伸断口形貌 |
Fig.4 Morphology of fracture surfaces of SLM GH4169 alloy after tensile tests at different temperatures (a1~a2) 25 oC; (b1~b2) 450 oC; (c1~c2) 500 oC; (d1~d2) 600 oC; (e1~e2) 650 oC |
![]() |