表4 三种试样的微观组织类型、片层大小、晶粒尺寸
Table 4 Microstructure type, lamellar size and grain size of samples
SamplesCooling processMicrostructureLayers spacing / nmGrain size / μm
1#Air coolingPearlite324.620.73
2#Wind CoolingPearlite133.913.38