尖晶石型无钴(Cr0.2Fe0.2Mn0.2Ni0.2X0.2)3O4 高熵氧化物的制备及其储锂性能
邵霞, 鲍梦凡, 陈诗洁, 林娜, 檀杰, 冒爱琴

Preparation and Lithium Storage Performance of Spinel-type Cobalt-free (Cr0.2Fe0.2Mn0.2Ni0.2X0.2)3O4 High-entropy Oxide
SHAO Xia, BAO Mengfan, CHEN Shijie, LIN Na, TAN Jie, MAO Aiqin
表2 样品的同种金属元素不同价态之比
Table 2 Ratio of different valence states of the same metal element in the samples
SamplesCr3+/Cr6+Fe2+/Fe3+Mn3+/Mn4+Ni2+/Ni3+Co2+/Co3+
4MCo55.8/44.250.9/49.171.7/28.359.2/40.846.4/53.6
4MK42.3/57.762.8/37.272.5/27.559.2/40.8K+
4MMg60.2/39.853.9/46.167.1/32.952.6/47.4Mg2+
4MZn71.7/28.351.4/48.681.3/18.754.7/45.3Zn2+