尖晶石型无钴(Cr0.2Fe0.2Mn0.2Ni0.2X0.2)3O4 高熵氧化物的制备及其储锂性能 |
邵霞, 鲍梦凡, 陈诗洁, 林娜, 檀杰, 冒爱琴 |
Preparation and Lithium Storage Performance of Spinel-type Cobalt-free (Cr0.2Fe0.2Mn0.2Ni0.2X0.2)3O4 High-entropy Oxide |
SHAO Xia, BAO Mengfan, CHEN Shijie, LIN Na, TAN Jie, MAO Aiqin |
图6 4MZn电极在不同扫速下的CV曲线、lg(ip)与lg(v)的关系曲线、1 mV·s-1时赝电容(蓝色区域)和扩散(红色区域)控制的贡献率以及不同扫描速率的赝电容贡献率 |
Fig.6 CV curves at different scan rates (a), linear relationship between peak current and scan rate (b), the overall current signal (solid red line) and pseudocapacitive current (shaded blue region) at 1 mV·s-1 scan rate (c), Pseudo-capacitive contribution (d) of the eletrodes at different scan rates |
![]() |