尖晶石型无钴(Cr0.2Fe0.2Mn0.2Ni0.2X0.2)3O4 高熵氧化物的制备及其储锂性能
邵霞, 鲍梦凡, 陈诗洁, 林娜, 檀杰, 冒爱琴

Preparation and Lithium Storage Performance of Spinel-type Cobalt-free (Cr0.2Fe0.2Mn0.2Ni0.2X0.2)3O4 High-entropy Oxide
SHAO Xia, BAO Mengfan, CHEN Shijie, LIN Na, TAN Jie, MAO Aiqin
图2 4MCo、4MK、4MMg和4MZn样品的N2吸/脱附等温线和BJH孔径分布
Fig.2 N2 adsorption-desorption isothermal curves, BJH pore size distribution of the samples (a) 4MCo, (b) 4MK, (c) 4MMg and (d) 4MZn