尖晶石型无钴(Cr0.2Fe0.2Mn0.2Ni0.2X0.2)3O4 高熵氧化物的制备及其储锂性能
邵霞, 鲍梦凡, 陈诗洁, 林娜, 檀杰, 冒爱琴

Preparation and Lithium Storage Performance of Spinel-type Cobalt-free (Cr0.2Fe0.2Mn0.2Ni0.2X0.2)3O4 High-entropy Oxide
SHAO Xia, BAO Mengfan, CHEN Shijie, LIN Na, TAN Jie, MAO Aiqin
图1 样品的XRD谱和XRD谱的局部放大图、样品的SEM照片以及4MCo、4MK、4MMg、4MZn和4MZn各元素的EDS图
Fig.1 XRD patterns of the samples (a) and enlarge patterns (b) and SEM images of the samples ((c) 4MCo, (d) 4MK, (e) 4MMg, (f, g) 4MZn) and (h) EDS images of 4MZn