在铝液中热循环H13钢的软化行为 |
娄伟冬, 赵海东, 王果 |
Softening Behavior of H13 Steel by Thermal Cycling between Molten ADC12 Al-alloy and Spray Cooling Chamber |
LOU Weidong, ZHAO Haidong, WANG Guo |
图7 H13钢循环5000次时的EBSD图 |
Fig.7 IPF, misorientation boundaries and KAM maps of H13 (a~c) original, (d~f) 670oC, (g~i) 700oC, (j~l) 730oC. Misorientation boundaries are colored as follows: red, 2°~5°; green, 5°~15°; blue, > 15° |
![]() |