时效处理对Fe-12Mn-8Al-1C-3Cu轻质钢的组织演变和力学性能的影响 |
| 刘加晓, 胡晓, 丁桦 |
|
Effect of Aging Treatment on Microstructure Evolution and Mechanical Properties of Fe-12Mn-8Al-1C-3Cu Lightweight Steel |
| LIU Jiaxiao, HU Xiao, DING Hua |
| 图6 实验钢在550℃时效10min后不同量变形后的变形组织TEM形貌 |
| Fig.6 TEM morphology of deformation structure of the experimental steel aged at 550oC for 10 min with different deformation extents (a) 5 %; (b) 10%; (c) 20%; (d) 30%; (e) 40% |
|