表10 Spearman等级相关分析结果
Table 10 Results of Spearman correlation analysis
PtotalPCO2pHTRctIcorr
Ptotalr1.0000.0000.0000.0000.147-0.211
P-1.0001.0001.0000.6020.451
PCO2r0.0001.0000.2320.000-0.623*0.692**
P1.000-0.4051.0000.0130.004
pHr0.0000.2321.0000.000-0.0780.085
P1.0000.405-1.0000.7810.765
Tr0.0000.0000.0001.000-0.692**0.633*
P1.0001.0001.000-0.0040.011
Rctr0.147-0.623*-0.078-0.692**1.000-0.986**
P0.6020.0130.7810.004-0.000
Icorrr-0.2110.692**0.0850.633*-0.986**1.000
P0.4510.0040.7650.0110.000-