J55钢在模拟CO2 注入井环空环境中的关键性腐蚀因素
崔怀云, 刘智勇, 卢琳

Critical Corrosion Factors for J55 Tubing Steel in a Simulated Annulus Environment of CO2 Injection Well
CUI Huaiyun, LIU Zhiyong, LU Lin
表2 油田水介质的成分
Table 2 Chemical composition of oilfield water
CompositionValue
Sulfate / mg·L-13000~15000
NaHCO3 / mg·L-1150~1000
KCl / mg·L-112000~15000
NaCl / mg·L-112000~15000
Inhibitor / mg·L-150~200
PCO2 / MPa4.00