氮磷共掺杂石墨烯的制备及水性复合涂层的耐蚀性能
|
李玉峰, 冯峰, 刘世博, 刘丽爽, 高晓辉
|
Preparation of Nitrogen and Phosphorus Co-doped Graphene Oxide and Corrosion Resistance of Waterborne Composite Coatings NPGO/Epoxy Resin
|
LI Yufeng, FENG Feng, LIU Shibo, LIU Lishuang, GAO Xiaohui
|
|
表2 EIS拟合数据
|
Table 2 Fitted data of EIS in Fig.9
|
|
Sample | Rs / Ω·cm2 | Rc / Ω·cm2 | CPEc | Rct / Ω·cm2 | CPEdl |
---|
Y0 / Ω·cm-2·s n | nc | Y0 / Ω·cm-2·s n | nc |
---|
EP | 35673 | 1.32 × 106 | 8.12 × 10-9 | 1.442 | 3.72 × 106 | 4.25 × 10-9 | 0.7936 | GO/EP | 28254 | 1.03 × 108 | 1.35 × 10-10 | 0.9358 | 1.04 × 107 | 6.13 × 10-10 | 0.8393 | NGO/EP | 32261 | 2.61 × 108 | 4.02 × 10-10 | 0.7754 | 3.97 × 107 | 2.66 × 10-11 | 1.986 | PGO/EP | 26477 | 2.52 × 108 | 2.65 × 10-10 | 0.9364 | 2.78 × 107 | 1.93 × 10-10 | 0.9238 | NPGO/EP | 32870 | 3.98 × 108 | 2.39 × 10-10 | 0.8145 | 4.41 × 107 | 2.22 × 10-10 | 1.071 |
|
|
|