316L钢表面低活性Fe-Al涂层的制备
陈继弘, 王永利, 熊良银, 宋立新

Preparation of Low Activity Fe-Al Coating on 316L Steel Surface
CHEN Jihong, WANG Yongli, XIONG Liangyin, SONG Lixin
图10 在不同温度渗铝不同时间316L管内壁的Fe-Al涂层的截面形貌的BSE图片
Fig.10 BSE images of the cross-sectional morphology of Fe-Al coatings aluminized on the inner wall of 316L tubes at different temperature for different time (a) 700oC/6 h; (b) 750oC/6 h; (c) 800oC/3 h; (d) 800oC/6 h; (e) 800oC/9 h