中温热处理对Ti65合金淬火组织及室温拉伸性能的影响
谭海兵, 臧健, 梁弼宁, 刘建荣, 王清江, 赵子博, 李文渊

Effect of Medium Heat Treatment on Quenched Micro-structure and Tensile Properties of Ti65 Alloy
TAN Haibing, ZANG Jian, LIANG Bining, LIU Jianrong, WANG Qingjiang, ZHAO Zibo, LI Wenyuan
表2 拉伸性能样品的热处理制度
Table 2 Heat treatment scheme of Ti65 alloy for tensile test
Solution treatmentMedium temperature treatmentsAging treatment
1030℃/2 h, WQAs-quenched700℃/5 h, AC
800℃/10, 20, 40, 60 min, WQ
850℃/10, 20, 40, 60 min,WQ
900℃/20, 40, 60 min, WQ
950℃/20, 40, 60 min, WQ