中温热处理对Ti65合金淬火组织及室温拉伸性能的影响 |
谭海兵, 臧健, 梁弼宁, 刘建荣, 王清江, 赵子博, 李文渊 |
Effect of Medium Heat Treatment on Quenched Micro-structure and Tensile Properties of Ti65 Alloy |
TAN Haibing, ZANG Jian, LIANG Bining, LIU Jianrong, WANG Qingjiang, ZHAO Zibo, LI Wenyuan |
图6 中温热处理后Ti65合金中α2相形貌的变化 |
Fig.6 TEM microstructure of α2 phase in Ti65 alloy heat-treated at (a) 1030℃/2 h, WQ+700℃/5 h, AC; (b) 1030℃/2 h, WQ+800℃/20 min, WQ; (c) 1030℃/2 h, WQ+800℃/20 min, WQ+700℃/5 h, AC; (d) 1030℃/2 h, WQ+850℃/20 min, WQ; (e) 1030℃/2 h, WQ+900℃/20 min, WQ; (f) super lattice diffraction spots from α2 phase precipitated in α phase in Fig.7b. Black indices belong to α, and red those belong to α2 phase |
![]() |