纳米多孔Fe-Si-B-P的脱合金制备及其电化学性能
赖祥晔, 翁楠, 池昱晨, 秦凤香

Formation and Electrochemical Properties of Nanoporous Fe-Si-B-P by Dealloying
LAI Xiangye, WENG Nan, CHI Yuchen, QIN Fengxiang
图8 在773 K热处理的Fe76Si9B10P5合金分别在0.005、0.01和0.05 mol/L的H2SO4溶液中脱合金处理600、1800、3600 s后所得样品的SEM照片
Fig.8 SEM morphologies of Fe76Si9B10P5 alloys annealed at 773 K after dealloying in 0.005 mol/L (a), 0.01 mol/L (b), 0.05 mol/L (c) H2SO4 solutions for 600 s (a1~a3), 1800 s (b1~b3), 3600 s (c1~c3)