一种6Re/3Ru镍基单晶高温合金微观组织的稳定性和高温持久性能
陈瑞志, 刘丽荣, 郭圣东, 张迈, 卢广先, 李远, 赵云松, 张剑

Microstructural Stability and Stress Rupture Property of a 6Re/3Ru Containing Nickel-based Single Crystal Superalloy
CHEN Ruizhi, LIU Lirong, GUO Shengdong, ZHANG Mai, LU Guangxian, LI Yuan, ZHAO Yunsong, ZHANG Jian
表2 用SEM-EDS能谱测量的断裂试样中μ相的成分
Table 2 Composition of μ phase in fractured specimen measured by SEM-EDS (mass fraction,%)
ReWNiCoTaHfCrMoRu
38.8519.2613.5311.288.864.512.710.680.32