退火温度对TC4钛合金热轧板材的显微组织、织构和力学性能影响 |
王伟, 周山琦, 宫鹏辉, 张浩泽, 史亚鸣, 王快社 |
Effect of Anneal Treatment on Microstructure, Texture and Mechanical Properties of TC4 Alloy Plates |
WANG Wei, ZHOU Shanqi, GONG Penghui, ZHANG Haoze, SHI Yaming, WANG Kuaishe |
图4 再结晶晶粒的分布 |
Fig.4 Recrystallization grain distribution map (a) original rolling state; (b) annealing at 750℃; (c) annealing at 800℃ (d) annealing at 850℃; (e) annealing at 900℃ (f) frequency of recrystallized grain distribution |
![]() |