热等静压对第三代单晶高温合金DD33显微组织和持久性能的影响
何禹锋, 王莉, 王栋, 王绍钢, 卢玉章, 谷阿山, 申健, 张健

Effect of Hot Isostatic Pressing on Microstructure of a Third-Generation Single Crystal Superalloy DD33
HE Yufeng, WANG Li, WANG Dong, WANG Shaogang, LU Yuzhang, GU Ashan, SHEN Jian, ZHANG Jian
图9 DD33合金HRS和HIP样品在1100℃/170 MPa下持久断口的组织形貌
Fig.9 Fracture morphology of (a, c, e) HRS and (b, d, f) HIP specimens after 1100℃/170 MPa (a, b) the fracture surfaces, (c, d) the longitudinal section OM morphologies, (e, f) the morphology of γ/γʹ microstructure