利用WBEEIS测试技术对管道缺陷区动态冲刷腐蚀行为的研究
杨留洋, 谭卓伟, 李同跃, 张大磊, 邢少华, 鞠虹

Dynamic Corrosion Behavior of Pipeline Defects Characterized by WBE and EIS Testing Techniques
YANG Liuyang, TAN Zhuowei, LI Tongyue, ZHANG Dalei, XING Shaohua, JU Hong
表1 缺陷试样不同排列耦合的阻值参数变化
Table 1 Fitting resistance parameters of the different zones of the defective sample
PositionRs/Ω·cm2Y0(Qf)/Ω-1 cm-2s nRf/Ω·cm2Y0(Qct)/Ω-1 cm-2s nRct/Ω·cm2
Upper 16.670×10-16.475×10-43.3095.762×10-314.41
Upper 25.281×10-14.645×10-33.0036.359×10-310.08
Defects6.973×10-15.264×10-33.6823.169×10-315.27
Lower 15.608×10-1--2.344×10-25.092
Lower 26.523×10-19.729×10-43.1336.353×10-314.58