表2 用不同方法制备Sm2Fe17N x 的氮化条件和性能
Table 2 Sm2Fe17N x prepared by different preparation process: nitriding conditions, physical and magnetic properties
Preparation methodNitridationMorphologyImpurityPropertiesReference

Temperature

/K

Time

/h

Atmosphere

Length

/μm

Ms

/emu·g-1

Mr

/emu·g-1

Hcj

/kOe

Jet-milling technique///1.30/16314712.7[39]
Strip casting technique700~80010~24N20.80α-Fe16015513.0[44]
Strip casting technique69335N20.76/14.2 (kGs)12.5 (kGs)13.0[45]

Reduction-diffusion process

(Polymerized complex)

70310N20.69///23.2[27]

Reduction-diffusion process

(Co-precipitation)

693/

NH3/H2

(1:2 Vol/Vol)

0.90/1259028.1[11]

Reduction-diffusion process

(Hydrothermal)

6931

NH3/H2

(1:2 Vol/Vol)

0.66/14010524.1[53]

Reduction-diffusion process

(Thermal decomposition)

873/

Melamine

(C3H6N6)

0.10/128/15.4[55]