分级固溶处理对8Cr4Mo4V钢的微观组织和硬度的影响 |
于兴福, 王士杰, 郑冬月, 王全振, 苏勇, 赵文增, 邢飞 |
Effect of Graded Solution Treatments on Microstructure and Hardness of 8Cr4Mo4V Steel |
YU Xingfu, WANG Shijie, ZHENG Dongyue, WANG Quanzhen, SU Yong, ZHAO Wenzeng, XING Fei |
图8 不同二级固溶处理后8Cr4Mo4V钢的等温淬火组织和回火组织 |
Fig.8 Isothermal quenched microstructure (a, c, e) and tempered microstructure (b, d, f) of 8Cr4Mo4V steel after different secondary solution treatments (a) and (b), 1080℃; (c) and (d), 1090℃; (e) and (f), 1100℃ |
![]() |