分级固溶处理对8Cr4Mo4V钢的微观组织和硬度的影响 |
于兴福, 王士杰, 郑冬月, 王全振, 苏勇, 赵文增, 邢飞 |
Effect of Graded Solution Treatments on Microstructure and Hardness of 8Cr4Mo4V Steel |
YU Xingfu, WANG Shijie, ZHENG Dongyue, WANG Quanzhen, SU Yong, ZHAO Wenzeng, XING Fei |
图6 不同初级固溶处理8Cr4Mo4V钢的回火组织 |
Fig.6 Tempered microstructure of the 8Cr4Mo4V steel treated by different primary solution treatments (a) 1000℃; (b) 1020℃; (c) 1050℃; (d) 1060℃ |
![]() |