固溶温度对Ti-4Al-6Mo-2V-5Cr-2Zr钛合金的组织和拉伸性能的影响
王圣元, 张浩宇, 周舸, 陈晓博, 陈立佳

Effect of Solution Treatment Temperature on Microstructure and Tensile Properties of Ti-4Al-6Mo-2V-5Cr-2Zr Alloy
WANG Shengyuan, ZHANG Haoyu, ZHOU Ge, CHEN Xiaobo, CHEN Lijia
图3 Ti-4Al-6Mo-2V-5Cr-2Zr合金在相变点以上固溶1 h后的EBSD-IPF图和相分布
Fig.3 EBSD-IPF images and phase distribution images of Ti-4Al-6Mo-2V-5Cr-2Zr alloy after solution treatment above phase transition temperature for 1 h at 810℃, EBSD-IPF (a); at 810℃, phase distribution (b); at 830℃, EBSD-IPF (c) and at 830℃, phase distribution (d)